李克智


的个人主页 http://teacher.nwpu.edu.cn/likezhi

基本信息 The basic information

李克智

材料学院

博士研究生毕业

工学博士

教授

材料科学与工程

工作经历 Work Experience

李克智 教授,博士生导师。主要从事热结构复合材料的制备工艺、抗氧化涂层及应用技术研究。主持和参加国家自然科学基金等科研项目20余项。

教育经历 Education Experience

教育教学 Education And Teaching

荣誉获奖 Awards Information

获国家技术发明二等奖1项(2)、国家自然科学二等奖1项(3),获国家级教学成果一等奖1项(5)、国家级教学成果二等奖1项(4)。获授权国家发明专利38项。发表学术论文200余篇,其中SCI收录90余篇。 

科学研究 Scientific Research

学术成果 Academic Achievements

学术文献 Academic Literature

1. 两种沥青炭的微观结构研究 , 2016,39(4),565-568 ,DOI:10.7673/j.issn.1006-2793.2016.04.021, ISSN:1006-2793
2. C/C复合材料不同基体炭的微观结构 , 2016,44(7),7-12 ,DOI:10.11868/j.issn.1001-4381.2016.07.002, ISSN:1001-4381
3. Carbon foam decorated with silver particles and in situ grown nanowires for effective electromagnetic interference shielding , Springer New York LLC,2016,51(17),7991-8004 ,DOI:10.1007/s10853-016-0068-4, ISSN:00222461
4. Effects of hypervelocity impact on ablation behavior of SiC coated C/C composites , Elsevier Ltd,2016,108,151-156 ,DOI:10.1016/j.matdes.2016.06.106, ISSN:02641275
5. HfC-SiC改性炭/炭复合材料在氧乙炔环境下的烧蚀性能 , 2015,,64-72 ,DOI:, ISSN:
6. 中间相沥青基C/C复合材料的微观结构与断裂韧性 , 2016,37(4),7-10 ,DOI:10.15926/j.cnki.issn1672-6871.2016.04.002, ISSN:1672-6871
7. Characterization of latticed SiC nanowires containing coating for carbon foam using carbonization activated pack cementation process , Elsevier Ltd,2016,682,695-705 ,DOI:10.1016/j.jallcom.2016.04.319, ISSN:09258388
8. Synthesis, characterization, and ceramization of a SiC-ZrC-C preceramic polymer precursor , SPRINGER,2015,50(7),2824-2831 ,DOI:10.1007/s10853-015-8840-4, ISSN:0022-2461
9. Electromagnetic interference shielding effectiveness of carbon foam containing in situ grown silicon carbide nanowires , Elsevier Ltd,2016,42(9),11330-11340 ,DOI:10.1016/j.ceramint.2016.04.054, ISSN:02728842
10. Use of waste rigid polyurethane for making carbon foam with fireproofing and anti-ablation properties , Elsevier Ltd,2016,101,332-339 ,DOI:10.1016/j.matdes.2016.04.008, ISSN:02641275
11. Micro-oxidation treatment to improve bonding strength of Sr and Na co-substituted hydroxyapatite coatings for carbon/carbon composites , Elsevier,2016,378,136-141 ,DOI:10.1016/j.apsusc.2016.03.216, ISSN:01694332
12. Morphology-controlled fabrication of Co3O4nanostructures and their comparative catalytic activity for oxygen evolution reaction , Elsevier Ltd,2016,680,146-154 ,DOI:10.1016/j.jallcom.2016.04.084, ISSN:09258388
13. A dense and strong bonding collagen film for carbon/carbon composites , ELSEVIER SCIENCE BV,2015,347,307-314 ,DOI:10.1016/j.apsusc.2015.04.081, ISSN:0169-4332
14. Molybdenum Trioxide Dihydrate-Graphene Composite for Electrochemical Detection of Thiourea Molecule , World Scientific Publishing Co. Pte Ltd,2016,11(3) ,DOI:10.1142/S1793292016500363, ISSN:17932920
15. A novel combination of simple foaming and freeze-drying processes for making carbon foam containing multiwalled carbon nanotubes , Elsevier Ltd,2016,42(7),8980-8989 ,DOI:10.1016/j.ceramint.2016.01.131, ISSN:02728842
16. Effect of ZrO2 morphology on the ablation resistance of carbon/carbon composites containing ZrC prepared by the carbothermal reduction reaction , PERGAMON-ELSEVIER SCIENCE LTD,2016,102,405-412 ,DOI:10.1016/j.corsci.2015.10.033, ISSN:0010-938X
17. Ablation resistance of HfC-SiC coating prepared by supersonic atmospheric plasma spraying for SiC-coated C/C composites , ELSEVIER SCI LTD,2016,42(4),4768-4774 ,DOI:10.1016/j.ceramint.2015.11.161, ISSN:0272-8842
18. Ablation behavior of rare earth La-modified ZrC coating for SiC-coated carbon/carbon composites under an oxyacetylene torch , PERGAMON-ELSEVIER SCIENCE LTD,2016,104,61-70 ,DOI:10.1016/j.corsci.2015.11.030, ISSN:0010-938X
19. Effect of pH on crystallization of nanocrystalline zirconia in a microwave-hydrothermal process , Wuhan Ligong Daxue,2016,31(1),68-73 ,DOI:10.1007/s11595-016-1332-9, ISSN:10002413
20. La and F co-substituted hydroxyapatite bioactive coating reinforced by SiC nanowire/ZrO2 hybrid materials for carbon/carbon composites , ELSEVIER SCI LTD,2016,42(2),2164-2169 ,DOI:10.1016/j.ceramint.2015.09.170, ISSN:0272-8842
21. Preparation of high texture three-dimensional braided carbon/carbon composites by pyrolysis of ethanol and methane , ELSEVIER SCI LTD,2016,42(2),2887-2891 ,DOI:10.1016/j.ceramint.2015.10.059, ISSN:0272-8842
22. Three-dimensional carbon/carbon composites with vertically aligned carbon nanotubes: Providing direct and indirect reinforcements to the pyrocarbon matrix , ELSEVIER SCI LTD,2016,92,120-128 ,DOI:10.1016/j.matdes.2015.12.036, ISSN:0261-3069
23. Improving mechanical strength and thermal shock resistance of SiC/zinc aluminum silicate joint by electrophoretic deposited multi-walled carbon nanotubes , ELSEVIER SCI LTD,2016,94,417-423 ,DOI:10.1016/j.matdes.2016.01.061, ISSN:0261-3069
24. Sublimation and oxidation zone ablation behavior of carbon/carbon composites , ELSEVIER SCI LTD,2015,41(10),13751-13758 ,DOI:10.1016/j.ceramint.2015.08.043, ISSN:0272-8842
25. Ablation resistance of SiC-HfC-ZrC multiphase modified carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2016,103,1-9 ,DOI:10.1016/j.corsci.2015.06.037, ISSN:0010-938X
26. Response of MG63 Osteoblast-like Cells on Pyrolytic Carbon Coated Carbon/Carbon Composites , TRANS TECH PUBLICATIONS LTD,2009,620-622,579-582 ,DOI:10.4028/www.scientific.net/MSF.620-622.579, ISSN:0255-5476
27. AN Yb2Si2O7 OXIDATION RESISTANCE COATING FOR C/C COMPOSITES BY SUPERSONIC PLASMA SPRAY , AMER CERAMIC SOC,2011,32(3),85-90 ,DOI:, ISSN:0196-6219
28. 碳纤维增强纸基摩擦材料磨损机理研究 , 2011,(中国北京),400-405 ,DOI:, ISSN:
29. Biotribology behavior of ultra-high molecular weight polyethylene against carbon/carbon composites used for hip joint replacement , TRANS TECH PUBLICATIONS LTD,2011,685,327-330 ,DOI:10.4028/www.scientific.net/MSF.685.327, ISSN:0255-5476
30. Density, microstructure and mechanical property of large-scale C/C composites prepared by thermal gradient CVI , TRANS TECH PUBLICATIONS LTD,2012,535-537,139-143 ,DOI:10.4028/www.scientific.net/AMR.535-537.139, ISSN:1022-6680
31. Microstructures and electrocatalytic properties of nitrogen doped graphene synthesized by pyrolysis of metal tetrapyrazinoporphyrazine , TRANS TECH PUBLICATIONS LTD,2013,275-277,1762-1768 ,DOI:10.4028/www.scientific.net/AMM.275-277.1762, ISSN:1660-9336
32. Growth and microstructure of submicro-scaled graphitic flakes on carbon fibers by catalytic chemical vapor deposition , TRANS TECH PUBLICATIONS LTD,2013,275-277,1746-1750 ,DOI:10.4028/www.scientific.net/AMM.275-277.1746, ISSN:1660-9336
33. Catalytic activity of tetranitro-copper phthalocyanine supported on carbon nanotubes towards oxygen reduction reaction , TRANS TECH PUBLICATIONS LTD,2013,706-708,15-19 ,DOI:10.4028/www.scientific.net/AMR.706-708.15, ISSN:1022-6680
34. 微通道换热器用泡沫炭的制备及改性 , 2014,33(2),39-44 ,DOI:, ISSN:1001-3741
35. 化学液相气化沉积C/C复合材料的性能研究 , 2007,41(5),557-561 ,DOI:10.3321/j.issn:0253-987X.2007.05.012, ISSN:0253-987X
36. 碳泡沫先驱体酚醛泡沫制备工艺研究 , 2003,19(4),331-334 ,DOI:10.3969/j.issn.1006-4710.2003.04.008, ISSN:1006-4710
37. 碳纤维增强水泥基复合材料(CFRC)的压敏特性 , 2011,32(1),47-50 ,DOI:10.3969/j.issn.1671-6833.2011.01.012, ISSN:1671-6833
38. 炭/炭复合材料热梯度CVI工艺中温度场的数值模拟 , 2006,(z1),326-328,333 ,DOI:10.3969/j.issn.1001-4381.2006.z1.087, ISSN:1001-4381
39. 热梯度CVI工艺制备炭/炭复合材料管型件 , 2006,(z1),345-348 ,DOI:10.3969/j.issn.1001-4381.2006.z1.092, ISSN:1001-4381
40. 短切碳纤维水泥砂浆的电磁波反射性能 , 2010,41(z1),89-93 ,DOI:, ISSN:1001-9731
41. Influence of silicon content on microstructure and antioxidation property of SiC coating for carbon-carbon composites , MANEY PUBLISHING,2007,23(4),253-256 ,DOI:10.1179/174329407X215221, ISSN:0267-0844
42. Si-W-Mo coating for SiC coated carbon/carbon composites against oxidation , ELSEVIER SCIENCE SA,2007,201(24),9598-9602 ,DOI:10.1016/j.surfcoat.2007.04.062, ISSN:0257-8972
43. A cordierite-mullite anti-oxidation coating for carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(13),2708-2710 ,DOI:10.1016/j.carbon.2007.08.017, ISSN:0008-6223
44. An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2008,46(1),179-182 ,DOI:10.1016/j.carbon.2007.10.022, ISSN:0008-6223
45. Multilayer oxidation resistant coating for SiC coated carbon/carbon composites at high temperature , ELSEVIER SCIENCE SA,2008,475(1-2),279-284 ,DOI:10.1016/j.msea.2007.04.053, ISSN:0921-5093
46. Study on the electromagnetic interference of CFRC composites by reflectivity , JOURNAL MATER SCI TECHNOL,2008,24(2),265-271 ,DOI:, ISSN:1005-0302
47. Multi-composition oxidation resistant coating for SiC-coated carbon/carbon composites at high temperature , ELSEVIER SCIENCE SA,2008,486(1-2),556-561 ,DOI:10.1016/j.msea.2007.09.042, ISSN:0921-5093
48. Vitreous joining of SiC-coated carbon/carbon composites , ELSEVIER SCIENCE BV,2008,62(16),2347-2350 ,DOI:10.1016/j.matlet.2007.11.100, ISSN:0167-577X
49. Silicon assistant carbothermal reduction for SiC powders , JOURNAL OF UNIV OF SCIENCE AND TECHNOLOGY BEIJING,2008,15(4),484-488 ,DOI:10.1016/S1005-8850(08)60091-2, ISSN:1005-8850
50. Large-scale synthesis and photoluminescence properties of hexagonal-shaped SiC nanowires , ELSEVIER SCIENCE SA,2008,462(1-2),271-274 ,DOI:10.1016/j.jallcom.2007.08.014, ISSN:0925-8388
51. SiC-Si-ZrSiO4 Multiphase Oxidation Protective Coating for Carbon/Carbon Composites , JOURNAL MATER SCI TECHNOL,2008,24(6),941-944 ,DOI:, ISSN:1005-0302
52. SiC/Si-W-Mo coating for protection of C/C composites at 1873 K , INT JOURNAL MINERALS METALLURGY & MATERIALS, EDITORIAL DEPT,2008,15(6),822-826 ,DOI:, ISSN:1005-8850
53. Effect of Si/Ta Ratio on the Microstructure and High Temperature Anti-Oxidation Property of SiC/TaSi2 Coating for Carbon/Carbon Composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2009,38,252-256 ,DOI:, ISSN:1002-185X
54. Oxidation protection of carbon/carbon composites with SiC/indialite coating for intermediate temperatures , ELSEVIER SCI LTD,2009,29(9),1803-1807 ,DOI:10.1016/j.jeurceramsoc.2008.11.003, ISSN:0955-2219
55. Joining of carbon/carbon composites for nuclear applications , SPRINGER,2009,44(14),3747-3750 ,DOI:10.1007/s10853-009-3501-0, ISSN:0022-2461
56. High-temperature property of carbon/carbon composite joints bonded with ternary Ti-Si-C compound , ELSEVIER SCIENCE SA,2009,480(2),747-749 ,DOI:10.1016/j.jallcom.2009.02.040, ISSN:0925-8388
57. Photoluminescence performance of SiC nanowires, whiskers and agglomerated nanoparticles synthesized from activated carbon , ELSEVIER SCIENCE BV,2009,41(8),1616-1620 ,DOI:10.1016/j.physe.2009.05.004, ISSN:1386-9477
58. Effect of HfC on the ablative and mechanical properties of C/C composites , ELSEVIER SCIENCE SA,2009,517(1-2),61-67 ,DOI:10.1016/j.msea.2009.03.040, ISSN:0921-5093
59. Carbon Nanotube-Templated Copper Phthalocyanine Derivative Assemblies via Solid-Phase Synthesis: Effects of Hydrogen Bond on the Structure of the Assemblies , AMER CHEMICAL SOC,2009,9(9),4136-4141 ,DOI:10.1021/cg900366k, ISSN:1528-7483
60. MG63 OSTEOBLAST-LIKE CELLS RESPONSE OF SiC COATING FOR CARBON/CARBON COMPOSITES , WORLD SCIENTIFIC PUBL CO PTE LTD,2009,16(5),683-687 ,DOI:10.1142/S0218625X09013165, ISSN:0218-625X
61. Effect of Mo/Si Ratio on the Microstructure and Oxidation Resistance of Si-Mo Coating for C/C Composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2009,38,109-112 ,DOI:, ISSN:1002-185X
62. Influence of the electronic configuration of the central metal ions on catalytic activity of metal phthalocyanines to Li/SOCl2 battery , ELSEVIER SCIENCE BV,2009,194(2,SI),1081-1084 ,DOI:10.1016/j.jpowsour.2009.06.047, ISSN:0378-7753
63. Synthesis of hybrid graphene carbon-coated nanocatalysts , ROYAL SOC CHEMISTRY,2010,20(38),8230-8232 ,DOI:10.1039/c0jm02187c, ISSN:0959-9428
64. Microstructure and ablation properties of zirconium carbide doped carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2010,48(2),344-351 ,DOI:10.1016/j.carbon.2009.09.035, ISSN:0008-6223
65. SiC nanowire-toughened MoSi2-SiC coating to protect carbon/carbon composites against oxidation , PERGAMON-ELSEVIER SCIENCE LTD,2010,52(5),1879-1882 ,DOI:10.1016/j.corsci.2010.01.031, ISSN:0010-938X
66. A hot-pressing reaction technique for SiC coating of carbon/carbon composites , ELSEVIER SCI LTD,2010,36(4),1463-1466 ,DOI:10.1016/j.ceramint.2010.01.002, ISSN:0272-8842
67. Densification and microstructure of carbon/carbon composites prepared by chemical vapor infiltration using ethanol as precursor , SCIENCE PRESS,2010,53(8),2232-2238 ,DOI:10.1007/s11431-009-3161-y, ISSN:1674-7321
68. ABLATION PROPERTY OF SiC-TaSi2 COATED CARBON/CARBON COMPOSITES , WORLD SCIENTIFIC PUBL CO PTE LTD,2010,17(5-6),487-491 ,DOI:10.1142/S0218625X10014302, ISSN:0218-625X
69. Carbon Nanotubes with Phthalocyanine-Decorated Surface Produced by NH3-Assisted Microwave Reaction and Their Catalytic Performance in Li/SOCl2 Battery , WILEY-BLACKWELL,2010,28(10),2059-2066 ,DOI:10.1002/cjoc.201090344, ISSN:1001-604X
70. Microstructure and growth mechanism of SiC nanowires with periodically fluctuating hexagonal prisms by CVD , ELSEVIER SCIENCE SA,2010,508(2),L36-L39 ,DOI:10.1016/j.jallcom.2010.08.127, ISSN:0925-8388
71. Oxidation Protective C/SiC/Si-SiC Multilayer Coating for Carbon/Carbon Composites Applying at 1873 K , JOURNAL MATER SCI TECHNOL,2010,26(12),1139-1142 ,DOI:10.1016/S1005-0302(11)60014-5, ISSN:1005-0302
72. Micro- and Nano-structure Characterization of Isotropic Pyrocarbon Obtained via Chemical Vapor Deposition in Hot Wall Reactor , JOURNAL MATER SCI TECHNOL,2010,26(12),1133-1138 ,DOI:10.1016/S1005-0302(11)60013-3, ISSN:1005-0302
73. Effect of brake pressure and brake speed on the tribological properties of carbon/carbon composites with different pyrocarbon textures , ELSEVIER SCIENCE SA,2010,270(1-2),95-103 ,DOI:10.1016/j.wear.2010.09.010, ISSN:0043-1648
74. The effect of zirconium carbide on ablation of carbon/carbon composites under an oxyacetylene flame , PERGAMON-ELSEVIER SCIENCE LTD,2011,53(1),105-112 ,DOI:10.1016/j.corsci.2010.09.028, ISSN:0010-938X
75. Large-scale production of graphene by microwave synthesis and rapid cooling , ROYAL SOC CHEMISTRY,2011,47(4),1166-1168 ,DOI:10.1039/c0cc03520c, ISSN:1359-7345
76. Modification of multi-walled carbon nanotubes with cobalt phthalocyanine: effects of the templates on the assemblies , ROYAL SOC CHEMISTRY,2011,21(4),1181-1186 ,DOI:10.1039/c0jm02156c, ISSN:0959-9428
77. Synthesis of MoS2 Nanosheets by Solid-State Reaction in CVD Furnace , TAYLOR & FRANCIS LTD,2011,128(1),125-129 ,DOI:10.1080/10584587.2011.576612, ISSN:1058-4587
78. Electrochemical performance of carbon nanotube-supported cobalt phthalocyanine and its nitrogen-rich derivatives for oxygen reduction , ELSEVIER SCIENCE BV,2011,335(1-2),89-96 ,DOI:10.1016/j.molcata.2010.11.018, ISSN:1381-1169
79. Effects of air oxidation on mesophase pitch-based carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2011,49(4),1416-1422 ,DOI:10.1016/j.carbon.2010.12.009, ISSN:0008-6223
80. Ablation of the carbon/carbon composite nozzle-throats in a small solid rocket motor , PERGAMON-ELSEVIER SCIENCE LTD,2011,49(4),1208-1215 ,DOI:10.1016/j.carbon.2010.11.037, ISSN:0008-6223
81. Graphite nanosheets doped with Fe, Ni, and N, synthesized in one step, and their unique magnetic performance , PERGAMON-ELSEVIER SCIENCE LTD,2011,151(8),643-646 ,DOI:10.1016/j.ssc.2011.01.020, ISSN:0038-1098
82. The influence of deposition temperature on the microstructure of isotropic pyrocarbon obtained by hot-wall chemical vapor deposition , SPRINGER,2011,46(10),3632-3638 ,DOI:10.1007/s10853-011-5279-0, ISSN:0022-2461
83. Densification behavior and microstructure of carbon/carbon composites prepared by chemical vapor infiltration from xylene at temperatures between 900 and 1250 degrees C , PERGAMON-ELSEVIER SCIENCE LTD,2011,49(7),2561-2570 ,DOI:10.1016/j.carbon.2011.02.046, ISSN:0008-6223
84. Oxidation protection of C/SiC coated carbon/carbon composites with Si-Mo coating at high temperature , PERGAMON-ELSEVIER SCIENCE LTD,2011,53(6),2075-2079 ,DOI:10.1016/j.corsci.2011.02.024, ISSN:0010-938X
85. Mechanical properties improvement of carbon/carbon composites by two different matrixes , SPRINGER,2011,46(13),4667-4674 ,DOI:10.1007/s10853-011-5373-3, ISSN:0022-2461
86. Thermal fatigue behavior of C/C composites modified by SiC-MoSi2-CrSi2 coating , ELSEVIER SCIENCE SA,2011,509(31),8111-8115 ,DOI:10.1016/j.jallcom.2011.05.068, ISSN:0925-8388
87. Influence of SiC nanowires on the properties of SiC coating for C/C composites between room temperature and 1500 degrees C , PERGAMON-ELSEVIER SCIENCE LTD,2011,53(9),3048-3053 ,DOI:10.1016/j.corsci.2011.05.046, ISSN:0010-938X
88. C/SiC/Si-Mo-B/glass multilayer oxidation protective coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2011,206(2-3),492-496 ,DOI:10.1016/j.surfcoat.2011.07.085, ISSN:0257-8972
89. C/SiC/MoSi2-Si multilayer coatings for carbon/carbon composites for protection against oxidation , PERGAMON-ELSEVIER SCIENCE LTD,2011,53(11),3840-3844 ,DOI:10.1016/j.corsci.2011.07.036, ISSN:0010-938X
90. Synthesis of centimeter-scale ultra-long SiC nanowires by simple catalyst-free chemical vapor deposition , ELSEVIER SCIENCE BV,2011,335(1),160-164 ,DOI:10.1016/j.jcrysgro.2011.09.021, ISSN:0022-0248
91. Microstructure and mechanical properties of carbon/carbon composites doped with LaCl3 , ELSEVIER SCIENCE SA,2011,529(1),177-183 ,DOI:10.1016/j.msea.2011.09.015, ISSN:0921-5093
92. Improvement in toughness of carbon/carbon composites using multiple matrixes , ELSEVIER SCIENCE SA,2011,530(1),57-62 ,DOI:10.1016/j.msea.2011.09.038, ISSN:0921-5093
93. SiC coating toughened by SiC nanowires to protect C/C composites against oxidation , ELSEVIER SCI LTD,2012,38(1),189-194 ,DOI:10.1016/j.ceramint.2011.05.159, ISSN:0272-8842
94. Nano/micro-sized calcium phosphate coating on carbon/carbon composites by ultrasonic assisted electrochemical deposition , WILEY-BLACKWELL,2012,44(1),21-28 ,DOI:10.1002/sia.3764, ISSN:0142-2421
95. Nitrogen-doped carbon nanotubes synthesized by pyrolysis of nitrogen-rich metal phthalocyanine derivatives for oxygen reduction , ROYAL SOC CHEMISTRY,2012,22(35),18230-18236 ,DOI:10.1039/c2jm33568a, ISSN:0959-9428
96. PREPARATION OF YTTRIUM ALUMINUM GARNET FIBERS BY THE SOL-GEL METHOD , INST CHEMICAL TECHNOLOGY, DEPT GLASS CERAMICS,2012,56(3),187-190 ,DOI:, ISSN:0862-5468
97. Effect of SiC Nanowires on the Mechanical and Oxidation Protective Ability of SiC Coating for C/C Composites , WILEY-BLACKWELL,2012,95(2),739-745 ,DOI:10.1111/j.1551-2916.2011.04979.x, ISSN:0002-7820
98. Coefficients of thermal expansion of low texture and isotropic pyrocarbon deposited on stationary substrates , ELSEVIER SCIENCE BV,2012,68,68-70 ,DOI:10.1016/j.matlet.2011.10.012, ISSN:0167-577X
99. Texture characterization and mechanical properties of pyrocarbon obtained by chemical vapor deposition at 1450-1550 degrees C , ELSEVIER SCIENCE SA,2012,539,1-6 ,DOI:10.1016/j.msea.2011.10.046, ISSN:0921-5093
100. Strong-bonding calcium phosphate coatings on carbon/carbon composites by ultrasound-assisted anodic oxidation treatment and electrochemical deposition , ELSEVIER SCIENCE BV,2012,258(12),5117-5125 ,DOI:10.1016/j.apsusc.2012.01.144, ISSN:0169-4332
101. Growth mechanism of silica nanowires without a metal catalyst via oxyacetylene torch ablation , ELSEVIER SCIENCE BV,2012,74,118-120 ,DOI:10.1016/j.matlet.2012.01.056, ISSN:0167-577X
102. Microstructure and ablation behaviors of integer felt reinforced C/C-SiC-ZrC composites prepared by a two-step method , ELSEVIER SCI LTD,2012,38(4),3419-3425 ,DOI:10.1016/j.ceramint.2011.12.054, ISSN:0272-8842
103. The study on joining carbon/carbon composites using Ti-Ni-Si compound , ELSEVIER SCIENCE SA,2012,547,12-18 ,DOI:10.1016/j.msea.2012.03.059, ISSN:0921-5093
104. Improving the oxidation resistance of carbon/carbon composites at low temperature by controlling the grafting morphology of carbon nanotubes on carbon fibres , PERGAMON-ELSEVIER SCIENCE LTD,2012,60,314-317 ,DOI:10.1016/j.corsci.2012.03.031, ISSN:0010-938X
105. Morphology, thermal response and anti-ablation performance of 3D-four directional pitch-based carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2012,61,134-142 ,DOI:10.1016/j.corsci.2012.04.036, ISSN:0010-938X
106. Grafting straight carbon nanotubes radially onto carbon fibers and their effect on the mechanical properties of carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2012,50(10),3949-3952 ,DOI:10.1016/j.carbon.2012.03.023, ISSN:0008-6223
107. Synthesis and photoluminescence of semiconductor ZnSe hollow microspheres by two-sourced evaporation , ELSEVIER SCIENCE SA,2012,531,86-90 ,DOI:10.1016/j.jallcom.2012.03.112, ISSN:0925-8388
108. Modeling of Generation of Uniform Metal Droplet During Drop-On-Demand Spray Forming , AMER SCIENTIFIC PUBLISHERS,2012,9(9,SI),1408-1412 ,DOI:10.1166/jctn.2012.2212, ISSN:1546-1955
109. C/SiC/Mo-Si-Cr multilayer coating for carbon/carbon composites against oxidation at high temperature , PERGAMON-ELSEVIER SCIENCE LTD,2012,63,410-414 ,DOI:10.1016/j.corsci.2012.05.023, ISSN:0010-938X
110. Surface characteristic and cell response of CVD SiC coating for carbon/carbon composites used for hip arthroplasty , WILEY-BLACKWELL,2012,44(10),1319-1323 ,DOI:10.1002/sia.5021, ISSN:0142-2421
111. Fabrication of Centimeter-scale Well-aligned SiC/SiO2 Core-shell Nanowires by Interlaminar Vapor-diffusion Reaction Method , BENTHAM SCIENCE PUBL LTD,2012,8(5),720-725 ,DOI:10.2174/157341312802884454, ISSN:1573-4137
112. Effects of a predeposited pyrocarbon layer on the microstructure and mechanical properties of carbon/carbon composites , ELSEVIER SCIENCE SA,2012,556,295-300 ,DOI:10.1016/j.msea.2012.06.090, ISSN:0921-5093
113. Electrodeposition of nanostructured calcium phosphate coating under magnetic field , MANEY PUBLISHING,2012,27(5),371-374 ,DOI:10.1179/1753555712Y.0000000026, ISSN:1066-7857
114. Na-doped hydroxyapatite coating on carbon/carbon composites: Preparation, in vitro bioactivity and biocompatibility , ELSEVIER SCIENCE BV,2012,263,163-173 ,DOI:10.1016/j.apsusc.2012.09.022, ISSN:0169-4332
115. Improved Surface Wettability of Water by Applying SiC/Ti6Al4V Coatings on Carbon/Carbon Composites , HINDAWI PUBLISHING CORPORATION,2013,2013 ,DOI:10.1155/2013/703610, ISSN:1687-8434
116. N-doped graphene analogue synthesized by pyrolysis of metal tetrapyridinoporphyrazine with high and stable catalytic activity for oxygen reduction , ROYAL SOC CHEMISTRY,2013,3(24),9344-9351 ,DOI:10.1039/c3ra41294f, ISSN:2046-2069
117. KINETICS OF GRAIN-GROWTH OF YTTRIUM ALUMINUM GARNET FIBERS PREPARED BY SOL-GEL METHOD , INST CHEMICAL TECHNOLOGY, DEPT GLASS CERAMICS,2013,57(4),285-289 ,DOI:, ISSN:0862-5468
118. Increasing mechanical strength retention rate of carbon/carbon composites after graphitization by grafting straight carbon nanotubes radially onto carbon fibers , ELSEVIER SCIENCE SA,2013,560,831-836 ,DOI:10.1016/j.msea.2012.10.046, ISSN:0921-5093
119. The preparation and mechanical properties of carbon-carbon/lithium-aluminum-silicate composite joints , ELSEVIER SCI LTD,2013,44,346-353 ,DOI:10.1016/j.matdes.2012.07.060, ISSN:0261-3069
120. Synthesis and Growth Mechanism of SiC/SiO2 Nanochains Heterostructure by Catalyst-Free Chemical Vapor Deposition , WILEY-BLACKWELL,2013,96(2),627-633 ,DOI:10.1111/jace.12005, ISSN:0002-7820
121. Partial transient liquid phase bonding of carbon/carbon composites using Ti-Ni-Al2O3-Si compound as interlayer , ELSEVIER SCIENCE SA,2013,550,57-62 ,DOI:10.1016/j.jallcom.2012.09.048, ISSN:0925-8388
122. The reinforcement and toughening of pyrocarbon-based carbon/carbon composite by controlling carbon nanotube growth position in carbon felt , ELSEVIER SCIENCE SA,2013,564,71-75 ,DOI:10.1016/j.msea.2012.11.074, ISSN:0921-5093
123. Ablation Behavior of ZrB2-Based Coating Prepared by Supersonic Plasma Spraying for SiC-Coated C/C Composites Under Oxyacetylene Torch , SPRINGER,2013,22(4),531-537 ,DOI:10.1007/s11666-013-9913-z, ISSN:1059-9630
124. X-ray diffraction and raman spectroscopy characterization of isotropic pyrocarbon obtained by hot wall chemical vapor deposition , JOURNAL WUHAN UNIV TECHNOLOGY,2013,28(2),358-361 ,DOI:10.1007/s11595-013-0695-4, ISSN:1000-2413
125. Microstructure and flexural properties of carbon/carbon composite with in-situ grown carbon nanotube as secondary reinforcement , ELSEVIER SCIENCE INC,2013,23(2),157-163 ,DOI:10.1016/j.pnsc.2013.03.001, ISSN:1002-0071
126. Ablation behavior and mechanism of C/C-ZrC-SiC composites under an oxyacetylene torch at 3000 degrees C , ELSEVIER SCI LTD,2013,39(4),4171-4178 ,DOI:10.1016/j.ceramint.2012.10.273, ISSN:0272-8842
127. Dynamic fatigue of two-dimensional carbon/carbon composites , ELSEVIER SCIENCE SA,2013,570,123-126 ,DOI:10.1016/j.msea.2013.01.073, ISSN:0921-5093
128. Electrochemical Performance of Dual Catalysts System Based on Nickel Phthalocyanine and Nano-Manganese Dioxide for O2 Reduction , TAYLOR & FRANCIS INC,2013,43(5),556-561 ,DOI:10.1080/15533174.2012.749893, ISSN:1553-3174
129. Effects of porous C/C density on the densification behavior and ablation property of C/C-ZrC-SiC composites , PERGAMON-ELSEVIER SCIENCE LTD,2013,57,161-168 ,DOI:10.1016/j.carbon.2013.01.059, ISSN:0008-6223
130. 3000℃氧-乙炔重复烧蚀后4D-炭/炭复合材料的剩余强度和热物理性能(英文) , ELSEVIER SCIENCE BV,2013,23(06),1661-1667 ,DOI:10.1016/S1003-6326(13)62645-X, ISSN:1003-6326
131. Effect of reaction temperature on crystallization of nanocrystalline zirconia synthesized by microwave-hydrothermal process , ELSEVIER SCIENCE SA,2013,561,23-27 ,DOI:10.1016/j.jallcom.2013.01.157, ISSN:0925-8388
132. The preparation and mechanical properties of carbon/carbon composite joints using Ti-Si-SiC-C filler as interlayer , ELSEVIER SCIENCE SA,2013,574,37-45 ,DOI:10.1016/j.msea.2013.03.007, ISSN:0921-5093
133. Microstructure and oxidation resistance of Si-Mo-B coating for C/SiC coated carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2013,72,150-155 ,DOI:10.1016/j.corsci.2013.03.015, ISSN:0010-938X
134. 弯曲载荷下纯净光滑层热解炭基2D-C/C复合材料的断裂机制(英文) , ELSEVIER SCIENCE BV,2013,23(07),2141-2146 ,DOI:10.1016/S1003-6326(13)62709-0, ISSN:1003-6326
135. Mechanical and thermophysical properties of carbon/carbon composites with hafnium carbide , ELSEVIER SCI LTD,2013,39(6),6769-6776 ,DOI:10.1016/j.ceramint.2013.02.006, ISSN:0272-8842
136. A novel method to fabricate isotropic pyrocarbon by densifying a multi-walled carbon nanotube preform by fixed-bed chemical vapor deposition , PERGAMON-ELSEVIER SCIENCE LTD,2013,59,547-550 ,DOI:10.1016/j.carbon.2013.03.044, ISSN:0008-6223
137. Increasing the Tensile Property of Unidirectional Carbon/Carbon Composites by Grafting Carbon Nanotubes onto Carbon Fibers by Electrophoretic Deposition , JOURNAL MATER SCI TECHNOL,2013,29(8),711-714 ,DOI:10.1016/j.jmst.2013.05.015, ISSN:1005-0302
138. Effect of heat flux on ablation behaviour and mechanism of C/C-ZrB2-SiC composite under oxyacetylene torch flame , PERGAMON-ELSEVIER SCIENCE LTD,2013,74,265-270 ,DOI:10.1016/j.corsci.2013.04.052, ISSN:0010-938X
139. Ablation in different heat fluxes of C/C composites modified by ZrB2-ZrC and ZrB2-ZrC-SiC particles , PERGAMON-ELSEVIER SCIENCE LTD,2013,74,159-167 ,DOI:10.1016/j.corsci.2013.04.038, ISSN:0010-938X
140. Microstructure and ablation resistance of ZrC nanostructured coating for carbon/carbon composites , ELSEVIER SCIENCE BV,2013,107,99-102 ,DOI:10.1016/j.matlet.2013.05.124, ISSN:0167-577X
141. Ablation resistance and thermal conductivity of carbon/carbon composites containing hafnium carbide , PERGAMON-ELSEVIER SCIENCE LTD,2013,75,169-175 ,DOI:10.1016/j.corsci.2013.05.029, ISSN:0010-938X
142. Oxidation resistant graded multiphase coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2013,232,821-826 ,DOI:10.1016/j.surfcoat.2013.06.105, ISSN:0257-8972
143. Microstructure and thermal conductivity of carbon/carbon composites containing zirconium carbide , SPRINGER,2013,48(21),7568-7573 ,DOI:10.1007/s10853-013-7572-6, ISSN:0022-2461
144. Dipotassium hydrogen phosphate as reducing agent for the efficient reduction of graphene oxide nanosheets , ACADEMIC PRESS INC ELSEVIER SCIENCE,2013,409,1-7 ,DOI:10.1016/j.jcis.2013.07.021, ISSN:0021-9797
145. Influence of compound mineral fiber on the properties of paper-based composite friction material , SAGE PUBLICATIONS LTD,2013,227(11),1241-1252 ,DOI:10.1177/1350650113487827, ISSN:1350-6501
146. Wear behavior of SiC nanowire-reinforced SiC coating for C/C composites at elevated temperatures , ELSEVIER SCI LTD,2013,33(15-16),2961-2969 ,DOI:10.1016/j.jeurceramsoc.2013.06.018, ISSN:0955-2219
147. TaB2-SiC-Si multiphase oxidation protective coating for SiC-coated carbon/carbon composites , ELSEVIER SCI LTD,2013,33(15-16),2953-2959 ,DOI:10.1016/j.jeurceramsoc.2013.06.028, ISSN:0955-2219
148. Carbon foam/hydroxyapatite coating for carbon/carbon composites: Microstructure and biocompatibility , ELSEVIER SCIENCE BV,2013,286,421-427 ,DOI:10.1016/j.apsusc.2013.09.110, ISSN:0169-4332
149. Compressive properties of carbon/carbon composites reinforced by carbon nanotubes with different orientations and lengths , PERGAMON-ELSEVIER SCIENCE LTD,2014,99,76-79 ,DOI:10.1016/j.vacuum.2013.04.022, ISSN:0042-207X
150. Influence of grain size on wear behavior of SiC coating for carbon/carbon composites at elevated temperatures , ELSEVIER SCI LTD,2014,53,412-418 ,DOI:10.1016/j.matdes.2013.07.046, ISSN:0261-3069
151. Tribological and mechanical properties of glass fiber reinforced paper-based composite friction material , ELSEVIER SCI LTD,2014,69,156-167 ,DOI:10.1016/j.triboint.2013.08.003, ISSN:0301-679X
152. Applying diamond like carbon layer on carbon/carbon composites and its effect on the deposition of hydroxyapatite coating , WILEY-BLACKWELL,2014,46(1),24-29 ,DOI:10.1002/sia.5341, ISSN:0142-2421
153. EFFECT OF ZIRCONIA ON CRYSTALLIZATION OF YTTRIUM ALUMINUM GARNET PRECURSOR GEL FIBERS , INST CHEMICAL TECHNOLOGY, DEPT GLASS CERAMICS,2014,58(2),118-122 ,DOI:, ISSN:0862-5468
154. SURFACE HYDROPHILIC MODIFICATION FOR CARBON/CARBON COMPOSITES AND ITS EFFECT ON THE BONDING STRENGTH OF HYDROXYAPATITE COATING , WORLD SCIENTIFIC PUBL CO PTE LTD,2014,21(1) ,DOI:10.1142/S0218625X14500164, ISSN:0218-625X
155. Effects of microstructures on the ablation behaviors of ZrC deposited by CVD , ELSEVIER SCIENCE SA,2014,240,450-455 ,DOI:10.1016/j.surfcoat2013.12.074, ISSN:0257-8972
156. The role of grafting force and surface wettability in interfacial enhancement of carbon nanotube/carbon fiber hierarchical composites , PERGAMON-ELSEVIER SCIENCE LTD,2014,69,239-246 ,DOI:10.1016/j.carbon.2013.12.020, ISSN:0008-6223
157. The effect of zirconium incorporation on the thermal stability and carbonized product of phenol-formaldehyde resin , ELSEVIER SCI LTD,2014,102(1),180-185 ,DOI:10.1016/j.polymdegradstab.2014.01.013, ISSN:0141-3910
158. Cyclic ablation behavior of C/C-ZrC-SiC composites under oxyacetylene torch , ELSEVIER SCI LTD,2014,40(4),5165-5171 ,DOI:10.1016/j.ceramint.2013.10.069, ISSN:0272-8842
159. Microstructure and growth mechanism of ZrO2 nanorod network via oxyacetylene torch ablation , ELSEVIER SCIENCE BV,2014,123,217-220 ,DOI:10.1016/j.matlet.2014.03.012, ISSN:0167-577X
160. Preparation of oxidation protective ZrB2-SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites , ELSEVIER SCIENCE SA,2014,247,61-67 ,DOI:10.1016/j.surfcoat.2014.03.017, ISSN:0257-8972
161. Electrophoretic deposition of carbon nanotubes onto carbon fiber felt for production of carbon/carbon composites with improved mechanical and thermal properties , PERGAMON-ELSEVIER SCIENCE LTD,2014,104,105-110 ,DOI:10.1016/j.vacuum.2014.01.024, ISSN:0042-207X
162. Synthesis, characterization and ceramization of a carbon-rich zirconium-containing precursor for ZrC ceramic , ELSEVIER SCI LTD,2014,40(5),7285-7292 ,DOI:10.1016/j.ceramint.2013.12.069, ISSN:0272-8842
163. ZrB2-SiC gradient oxidation protective coating for carbon/carbon composites , ELSEVIER SCI LTD,2014,40(5),7171-7176 ,DOI:10.1016/j.ceramint.2013.12.055, ISSN:0272-8842
164. Ablation mechanism of SiC coated C/C composites at 0 degrees angle in two flame conditions under an oxyacetylene flame , PERGAMON-ELSEVIER SCIENCE LTD,2014,84,1-10 ,DOI:10.1016/j.corsci.2014.03.009, ISSN:0010-938X
165. Graphene nanosheets synthesis via chemical reduction of graphene oxide using sodium acetate trihydrate solution , ELSEVIER SCIENCE SA,2014,193,132-138 ,DOI:10.1016/j.synthmet.2014.04.007, ISSN:0379-6779
166. In situ synthesis mechanism of ZrB2-ZrC-C composites , ELSEVIER SCI LTD,2014,40(7),10297-10302 ,DOI:10.1016/j.ceramint.2014.02.122, ISSN:0272-8842
167. Ultra-high temperature ceramic TaB2-TaC-SiC coating for oxidation protection of SiC-coated carbon/carbon composites , ELSEVIER SCI LTD,2014,40(7),9419-9425 ,DOI:10.1016/j.ceramint.2014.02.013, ISSN:0272-8842
168. Floating catalyst chemical vapor infiltration of nanofilamentous carbon reinforced carbon/carbon composites - Densification behavior and matrix microstructure , PERGAMON-ELSEVIER SCIENCE LTD,2014,75,353-365 ,DOI:10.1016/j.carbon.2014.04.014, ISSN:0008-6223
169. Microstructure and ablation resistance of carbon/carbon composites with a zirconium carbide rich surface layer , PERGAMON-ELSEVIER SCIENCE LTD,2014,85,160-166 ,DOI:10.1016/j.corsci.2014.04.013, ISSN:0010-938X
170. Effect of Bonding Temperature on the Microstructures and Strengths of C/C Composite/GH3044 Alloy Joints by Partial Transient Liquid-Phase (PTLP) Bonding with Multiple Interlayers , CHINESE ACAD SCIENCES, INST METAL RESEARCH,2014,27(4),663-669 ,DOI:10.1007/s40195-014-0090-y, ISSN:1006-7191
171. Effect of nickel introduced by electroplating on pyrocarbon deposition of carbon-fiber preforms , ELSEVIER SCIENCE INC,2014,27(4),1010-1014 ,DOI:10.1016/j.cja.2014.03.011, ISSN:1000-9361
172. Freezing-thawing effects on electromagnetic wave reflectivity of carbon fiber cement based composites , ELSEVIER SCI LTD,2014,64,288-292 ,DOI:10.1016/j.conbuildmat.2014.04.091, ISSN:0950-0618
173. Microstructure and thermal shock resistance of SiC/CNT-SiC double-layer coating for carbon/carbon composites , ELSEVIER SCI LTD,2014,40(8),13683-13689 ,DOI:10.1016/j.ceramint.2014.04.127, ISSN:0272-8842
174. A Na and Si co-substituted carbonated hydroxyapatite coating for carbon nanotubes coated carbon/carbon composites , ELSEVIER SCI LTD,2014,40(8),13123-13130 ,DOI:10.1016/j.ceramint.2014.05.015, ISSN:0272-8842
175. Microstructure and growth mechanism of ZrO2 nanorods network via oxyacetylene torch ablation (vol 123, pg 217, 2014) , ELSEVIER SCIENCE BV,2014,131,116-117 ,DOI:10.1016/j.matlet.2014.05.075, ISSN:0167-577X
176. Preparation and characterization of carbon/Sic nanowire/Na-doped carbonated hydroxyapatite multilayer coating for carbon/carbon composites , ELSEVIER SCIENCE BV,2014,313,85-92 ,DOI:10.1016/j.apsusc.2014.05.144, ISSN:0169-4332
177. TaxHf1-xB2-SiC multiphase oxidation protective coating for SiC-coated carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2014,87,479-488 ,DOI:10.1016/j.corsci.2014.07.016, ISSN:0010-938X
178. Monitoring the damage evolution of flexural fatigue in unidirectional carbon/carbon composites by electrical resistance change method , ELSEVIER SCI LTD,2014,68,248-252 ,DOI:10.1016/j.ijfatigue.2014.04.011, ISSN:0142-1123
179. Oxidation protective TaB2-SiC gradient coating to protect SiC-Si coated carbon/carbon composites against oxidation , ELSEVIER SCI LTD,2014,66,174-179 ,DOI:10.1016/j.compositesb.2014.05.021, ISSN:1359-8368
180. Improvement in thermal fatigue behavior of Si-Mo-Cr coated C/C composites through modification of the C/C-coating interface , ELSEVIER SCIENCE SA,2014,258,114-120 ,DOI:10.1016/j.surfcoat.2014.09.051, ISSN:0257-8972
181. Structure evolution and ablation behavior of ZrC coating on C/C composites under single and cyclic oxyacetylene torch environment , ELSEVIER SCI LTD,2014,40(10),16003-16014 ,DOI:10.1016/j.ceramint.2014.07.132, ISSN:0272-8842
182. Microstructure and Mechanical Properties of Multilayer-textured 2D Carbon/Carbon Composites , JOURNAL MATER SCI TECHNOL,2014,30(12),1202-1207 ,DOI:10.1016/j.jmst.2014.03.026, ISSN:1005-0302
183. Preparation of carbon/carbon composite by pyrolysis of ethanol and methane , ELSEVIER SCI LTD,2015,65,174-178 ,DOI:10.1016/j.matdes.2014.08.036, ISSN:0261-3069
184. Synthesis and characterization of nanobelt-shaped Na, F and carbonate multi-substituted hydroxyapatite , ELSEVIER SCIENCE BV,2015,138,48-51 ,DOI:10.1016/j.matlet.2014.09.009, ISSN:0167-577X
185. Double-layer TC4/Sr substituted hydroxyapatite bioactive coating for carbon/carbon composites , ELSEVIER SCI LTD,2015,41(1),427-435 ,DOI:10.1016/j.ceramint.2014.08.087, ISSN:0272-8842
186. Ablation behavior of CVD-ZrC coating under oxyacetylene torch environment with different heat fluxes , ELSEVIER SCI LTD,2015,48,108-114 ,DOI:10.1016/j.ijrmhm.2014.07.042, ISSN:0263-4368
187. Doping Effects on the Crystal Structure and Electrochemical Performance of LiFePO4/C , WILEY-BLACKWELL,2015,12(1),163-168 ,DOI:10.1111/ijac.12139, ISSN:1546-542X
188. Ablative and Mechanical Properties of C/C-ZrC Composites Prepared by Precursor Infiltration and Pyrolysis Process , JOURNAL MATER SCI TECHNOL,2015,31(1),77-82 ,DOI:10.1016/j.jmst.2014.01.015, ISSN:1005-0302
189. Preparation of oxidation protective Hf0.2Ta0.8B2-x-SiC coating by in-situ reaction method on SiC-coated carbon/carbon composites , ELSEVIER SCIENCE SA,2015,618,390-395 ,DOI:10.1016/j.jallcom.2014.08.185, ISSN:0925-8388
190. Enhancement of the oxidation resistance of C/C composites by depositing SiC nanowires onto carbon fibers by electrophoretic deposition , ELSEVIER SCIENCE SA,2015,618,336-342 ,DOI:10.1016/j.jallcom.2014.08.209, ISSN:0925-8388
191. Compressive and interlaminar shear properties of carbon/carbon composite laminates reinforced with carbon nanotube-grafted carbon fibers produced by injection chemical vapor deposition , ELSEVIER SCIENCE SA,2015,626,449-457 ,DOI:10.1016/j.msea.2014.12.044, ISSN:0921-5093
192. Oxidation protection of ultra-high temperature ceramic ZrxTa1-xB2-SiC/SiC coating prepared by in-situ reaction method for carbon/carbon composites , ELSEVIER SCI LTD,2015,35(3),897-907 ,DOI:10.1016/j.jeurceramsoc.2014.09.038, ISSN:0955-2219
193. Simultaneous improvements in flexural strength and ductility of carbon nanotube-doped carbon/carbon composites by depositing a pyrocarbon layer on carbon fibers , ELSEVIER SCI LTD,2015,41(2),1943-1949 ,DOI:10.1016/j.ceramint.2014.07.134, ISSN:0272-8842
194. Oxidation and erosion resistant property of SiC/Si-Mo-Cr/MoSi2 multi-layer coated C/C composites , ELSEVIER SCI LTD,2015,41(3),4101-4107 ,DOI:10.1016/j.ceramint.2014.11.105, ISSN:0272-8842
195. Electrodeposition of carbonate-containing hydroxyapatite on carbon nanotubes/carbon fibers hybrid materials for tissue engineering application , ELSEVIER SCI LTD,2015,41(3),4930-4935 ,DOI:10.1016/j.ceramint.2014.12.055, ISSN:0272-8842
196. Oxidation pre-treatment and electrophoretic deposition of SiC nanowires to improve the thermal shock resistance of SiC coating for C/C composites , ELSEVIER SCIENCE SA,2015,636,165-170 ,DOI:10.1016/j.jallcom.2015.02.075, ISSN:0925-8388
197. Multi-layer SiC/Mg and F co-substituted hydroxyapatite/chitosan bioactive coating for carbon fibers , ELSEVIER SCIENCE BV,2016,164,360-363 ,DOI:10.1016/j.matlet.2015.10.167, ISSN:0167-577X
198. Double layer ZrSi2-ZrC-SiC/SiC oxidation protective coating for carbon/carbon composites , MANEY PUBLISHING,2015,31(5),335-341 ,DOI:10.1179/1743294414Y.0000000428, ISSN:0267-0844
199. Influence of carbon nanotube extending length on pyrocarbon microstructure and mechanical behavior of carbon/carbon composites , ELSEVIER SCIENCE BV,2015,355,1020-1027 ,DOI:10.1016/j.apsusc.2015.07.198, ISSN:0169-4332
200. Microstructure and oxidation behavior of C/C-ZrB2-SiC composites coated with SiC coating at high temperature , PERGAMON-ELSEVIER SCIENCE LTD,2015,100,421-427 ,DOI:10.1016/j.corsci.2015.08.015, ISSN:0010-938X
201. Effect of high temperature heat treatment on the ablation of SiC-ZrB2-ZrC particles modified C/C composites in two heat fluxes , ELSEVIER SCIENCE SA,2015,621,18-25 ,DOI:10.1016/j.jallcom.2014.09.193, ISSN:0925-8388
202. Electrochemical sensing of ethylenediamine based on cuprous oxide/graphene hybrid structures , SPRINGER,2015,50(12),4288-4299 ,DOI:10.1007/s10853-015-8981-5, ISSN:0022-2461
203. ABLATION BEHAVIOR OF HfC COATING PREPARED BY SUPERSONIC PLASMA SPRAYING FOR SiC-COATED C/C COMPOSITES , ADCOTEC LTD,2015,24(5),113-118 ,DOI:, ISSN:0963-6935
204. Effect of vacuum thermal cyclic exposures on the carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2015,122,236-242 ,DOI:10.1016/j.vacuum.2015.10.001, ISSN:0042-207X
205. Microstructure and mechanical properties of carbon fiber reinforced multilayered (PyC-SiC)(n) matrix composites , ELSEVIER SCI LTD,2015,86,55-60 ,DOI:10.1016/j.matdes.2015.07.018, ISSN:0261-3069
206. Electromagnetic interference shielding effectiveness of carbon fiber reinforced multilayered (PyC-SiC)(n) matrix composites , ELSEVIER SCI LTD,2016,42(1),986-988 ,DOI:10.1016/j.ceramint.2015.08.131, ISSN:0272-8842
207. TiB2基复相陶瓷研究进展 , 2015,29(19),89-94 ,DOI:10.11896/j.issn.1005-023X.2015.019.016, ISSN:1005-023X
208. MG63 Osteoblast-like Cells Growth Behaviour on Carbon/Carbon Composites with Different Carbon Matrixes , EDITORIAL OFFICE CHINESE JOURNAL MECHANICAL ENGINEERING,2011,24(2),303-308 ,DOI:10.3901/CJME.2011.02.303, ISSN:1000-9345
209. 碳基及陶瓷基复合材料CVI工艺数值模拟的相关数学模型 , 1999,29(3),42-45 ,DOI:10.3969/j.issn.1007-2330.1999.03.009, ISSN:1007-2330
210. 短切炭纤维的CVI处理及其在CFRC中的分散性 , 2007,24(1),135-140 ,DOI:10.3321/j.issn:1000-3851.2007.01.023, ISSN:1000-3851
211. 工艺因素对C/C复合材料ICVI致密化的影响 , 2008,26(6),829 ,DOI:, ISSN:1673-2812
212. 二组元酞菁固相混合法裂解合成直立碳纳米管 , CHINESE CHEMICAL SOC,2009,25(6),951-955 ,DOI:10.3321/j.issn:1001-4861.2009.06.001, ISSN:1001-4861
213. 烧蚀产物ZrO2 对ZrC改性C/C复合材料烧蚀的影响 , SCIENCE PRESS,2009,24(5),943-947 ,DOI:10.3724/SP.J.1077.2009.00943, ISSN:1000-324X
214. 焦炭颗粒增强沥青基炭复合材料的组织结构 , 2009,32(1),57-60 ,DOI:10.3969/j.issn.1004-4248.2009.01.012, ISSN:1004-4248
215. 碳纤维增强水泥基复合材料(CFRC)的电学特性 , 2009,12(23),47-51 ,DOI:10.3321/j.issn:1005-023X.2009.23.011, ISSN:1005-023X
216. C/C复合材料与镍基高温合金连接接头断裂机制的研究 , 2009,32(3),45-48 ,DOI:10.3969/j.issn.1004-244X.2009.03.014, ISSN:1004-244X
217. 乙醇热解制备C/C复合材料工艺及组织结构研究 , 2010,40(8),965-972 ,DOI:, ISSN:1674-7259
218. 多涂层炭/炭复合材料抗1500℃燃气冲刷性能的研究 , SCIENCE CHINA PRESS,2010,25(4),279-284 ,DOI:10.1016/S1872-5805(09)60033-0, ISSN:1007-8827
219. CVD制备各向同性热解炭的微观结构表征及沉积机制研究 , 2010,29(4),21-24 ,DOI:10.3969/j.issn.1001-3741.2010.04.006, ISSN:1001-3741
220. 催化裂解天然气于碳毡内低成本合成碳纳米管 , 2010,24(24),86-90 ,DOI:, ISSN:1005-023X
221. 基于有限元的C/C燃气舵振动特性 , 2011,(1),12-15 ,DOI:, ISSN:1003-0999
222. 空气氧化处理的中间相沥青基炭/炭复合材料的组织和弯曲性能 , SCIENCE PRESS,2011,26(2),197-202 ,DOI:10.3724/SP.J.1077.2011.00197, ISSN:1000-324X
223. 碳化铪改性炭/炭复合材料喉衬的热化学烧蚀 , SCIENCE CHINA PRESS,2011,26(04),427-432 ,DOI:10.3724/SP.J.1077.2011.00427, ISSN:1000-324X
224. 碳/碳燃气舵热-结构数值模拟分析 , 2011,30(5),793-796,803 ,DOI:, ISSN:1003-8728
225. 碳纳米管含量对炭炭复合材料组织及力学性能的影响 , CHINESE CHEMICAL SOC,2011,27(5),1001-1007 ,DOI:, ISSN:1001-4861
226. 石墨粒度对纸基摩擦材料摩擦磨损性能的影响 , SCIENCE PRESS,2011,26(6),638-642 ,DOI:10.3724/SP.J.1077.2011.00638, ISSN:1000-324X
227. 炭/炭复合材料表面C/SiC/Si-Mo-Cr层复合防氧化涂层研究 , ELSEVIER SCIENCE BV,2012,27(2),105-110 ,DOI:10.1016/S1872-5805(12)60006-7, ISSN:1007-8827
228. 聚合物浸渍裂解法制备C/C-ZrC-SiC-ZrB_2复合材料及其性能研究 , SCIENCE PRESS,2013,28(06),605-610 ,DOI:10.3724/SP.J.1077.2013.12450, ISSN:1000-324X
229. 3000℃氧-乙炔重复烧蚀后4D-炭/炭复合材料的剩余强度和热物理性能 , 2013,23(6),1661-1667 ,DOI:, ISSN:1003-6326
230. 两种炭基C/C复合材料的微观结构及弯曲性能对比 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2013,36(3),398-402 ,DOI:10.7673/j.issn.1006-2793.2013.03.023, ISSN:1006-2793
231. 云母表面改性纸基摩擦材料的摩擦学性能* , 2013,38(7),16-21 ,DOI:10.3969/j.issn.0254-0150.2013.07.004, ISSN:0254-0150
232. 弯曲载荷下纯净光滑层热解炭基2D-C/C复合材料的断裂机制 , 2013,23(7),2141-2146 ,DOI:, ISSN:1003-6326
233. 炭/炭复合材料C/SiC/MoSi_2-SiC-Si抗氧化复合涂层 , 2013,23(7),2118-2122 ,DOI:, ISSN:1003-6326
234. 蛭石改性纸基摩擦材料的摩擦磨损性能研究 , 2013,27(16),113-117,122 ,DOI:10.3969/j.issn.1005-023X.2013.16.030, ISSN:1005-023X
235. CeO_2掺杂MAS中间层对C/C-LAS接头性能的影响 , SCIENCE PRESS,2013,28(12),1345-1348 ,DOI:10.3724/SP.J.1077.2013.13051, ISSN:1000-324X
236. FeSO4·7 H2 O粉末在炭布上原位催化生长多壁碳纳米管 , ELSEVIER SCIENCE BV,2013,28(6),421-427 ,DOI:10.1016/S1872-5805(13)60091-8, ISSN:1007-8827
237. 催化FBCVI制备碳纳米纤维增强碳/碳复合材料的组织与力学性能研究 , 2014,33(3),438-441 ,DOI:, ISSN:1003-8728
238. 浸渍用锆改性酚醛树脂的制备与表征 , 2014,42(8),76-78 ,DOI:, ISSN:1006-3536
239. ICVI工艺致密化C/C复合材料的数值模拟 , Journal of Solid Rocket Technology,2014,37(5),711-717 ,DOI:10.7673/j.issn.1006-2793.2014.05.024, ISSN:1006-2793
240. 基体改性对碳/碳复合材料烧蚀率影响的神经网络模拟 , 2003,37(3),249 ,DOI:, ISSN:0253-987X
241. 炭纤维对纸基摩擦材料摩擦磨损性能的影响 , 2004,24(6),555-559 ,DOI:10.3321/j.issn:1004-0595.2004.06.016, ISSN:1004-0595
242. 沥青基炭复合材料新型制备工艺的特征研究 , 2005,28(2),77-80 ,DOI:, ISSN:1004-4248
243. CLVI工艺制备C/C复合材料研究进展 , 2005,19(11),79 ,DOI:, ISSN:1005-023X
244. 碳纤维增强水泥基复合材料的发展与研究 , 2006,20(5),85-88 ,DOI:10.3321/j.issn:1005-023X.2006.05.024, ISSN:1005-023X
245. 化学液相气化沉积C/C复合材料的性能研究 , 2007,41(5),557-561 ,DOI:, ISSN:0253-987X
246. 医用炭/炭复合材料人工髋关节的磨损机理研究(英文) , SCIENCE CHINA PRESS,2010,25(09),999-1002 ,DOI:10.3724/SP.J.1077.2010.10144, ISSN:1000-324X
247. 带有SiC涂层的C/C复合材料的氧化行为 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2010,33(1),91-94 ,DOI:10.3969/j.issn.1006-2793.2010.01.022, ISSN:1006-2793
248. 碳/碳复合材料SiC-HfSi_2抗烧蚀复合涂层 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2010,38(2),352-356 ,DOI:, ISSN:0454-5648
249. Reflection properties against electromagnetic waves of chopped carbon fiber reinforced cement mortar , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2010,41(SUPPL. 1),89-93 ,DOI:, ISSN:10019731
250. 碳纳米管增强YAST微晶玻璃连接C/C复合材料与LAS陶瓷 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2010,33(4),459-462 ,DOI:10.3969/j.issn.1006-2793.2010.04.021, ISSN:1006-2793
251. 羰基铁粉-碳纤维水泥基复合材料的吸波性能 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2011,39(1),69-74 ,DOI:, ISSN:0454-5648
252. 纸基摩擦材料绿色制备工艺与摩擦磨损性能研究 , Science Press,2004,24(2),172-176 ,DOI:10.3321/j.issn:1004-0595.2004.02.018, ISSN:1004-0595
253. 石墨化处理对高压浸渍碳化碳/碳复合材料抗氧化性能的影响 , Chinese Ceramic Society,2004,32(12),1515-1519 ,DOI:10.3321/j.issn:0454-5648.2004.12.014, ISSN:0454-5648
254. 热处理温度对炭/炭复合材料性能的影响 , Editorial Office of Transactions of Materials and Heat Treatment,2005,26(1),1-4 ,DOI:10.3969/j.issn.1009-6264.2005.01.001, ISSN:1009-6264
255. 炭/炭复合材料用糠酮树脂先驱体的固化特性及动力学分析 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2012,35(1),123-126,132 ,DOI:10.3969/j.issn.1006-2793.2012.01.024, ISSN:1006-2793
256. 炭布叠层穿刺C/C复合材料螺栓连接件微观组织和力学性能 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2012,35(2),248-252 ,DOI:10.3969/j.issn.1006-2793.2012.02.022, ISSN:1006-2793
257. 化学气相沉积低温热解炭的微观组织结构与沉积模型 , ELSEVIER SCIENCE BV,2012,27(2),81-86 ,DOI:, ISSN:1007-8827
258. 碳化铪含量对C/C复合材料喉衬烧蚀性能的影响 , ELSEVIER SCIENCE BV,2012,27(4),311-314 ,DOI:, ISSN:1007-8827
259. 弯-弯疲劳加载对2D-C/C复合材料热膨胀性能的影响 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2012,35(5),665-669 ,DOI:, ISSN:1006-2793
260. HfB2 prepared by sol-gel method and its oxidation behavior , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi'an, 721014, China,2013,42(12),2594-2597 ,DOI:, ISSN:1002185X
261. 薄膜沸腾CVI双热源加热法制备C/C复合材料及其致密化特性 , ELSEVIER SCIENCE BV,2013,28(6),442-447 ,DOI:10.3969/j.issn.1007-8827.2013.06.011, ISSN:1007-8827
262. 碳纤维上原位生长碳纳米管对C/C复合材料弯曲性能的影响 , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2013,30(6),7-13 ,DOI:, ISSN:1000-3851
263. C/SiC陶瓷复合材料推力室的制备与性能表征 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2008,31(4),393-396,411 ,DOI:10.3969/j.issn.1006-2793.2008.04.021, ISSN:1006-2793
264. HfC改性C/C复合材料整体喉衬的烧蚀性能研究 , SCIENCE CHINA PRESS,2008,23(6),1155-1158 ,DOI:10.3321/j.issn:1000-324X.2008.06.014, ISSN:1000-324X
265. 表面热处理碳纤维及其增强水泥基复合材料的电磁屏蔽性能 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2008,36(10),1348-1355 ,DOI:10.3321/j.issn:0454-5648.2008.10.002, ISSN:0454-5648
266. C/C复合材料高温长寿命抗氧化复合涂层研究 , SCIENCE CHINA PRESS,2008,23(2),213-218 ,DOI:10.3321/j.issn:1000-324X.2008.02.002, ISSN:1000-324X
267. 冲中击损伤对C/C复合材料烧蚀性能的影响 , SCIENCE CHINA PRESS,2008,23(2),219-222 ,DOI:10.3321/j.issn:1000-324X.2008.02.003, ISSN:1000-324X
268. 碳/碳复合材料表面粗糙度对成骨细胞生长行为的影响 , SCIENCE CHINA PRESS,2008,23(2),341-345 ,DOI:10.3321/j.issn:1000-324X.2008.02.028, ISSN:1000-324X
269. C/C复合材料SiC-TaSi2/MoSi2抗氧化复合涂层研究 , SCIENCE CHINA PRESS,2008,44(3),331-335 ,DOI:10.3321/j.issn:0412-1961.2008.03.014, ISSN:0412-1961
270. 具有中间相沥青过渡层的炭/炭复合材料的微观结构与力学性能 , SCIENCE CHINA PRESS,2008,23(3),486-490 ,DOI:10.3321/j.issn:1000-324X.2008.03.014, ISSN:1000-324X
271. 碳/碳复合材料SiC-HfSi2-TaSi2抗烧蚀复合涂层 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2009,37(5),804-807 ,DOI:, ISSN:0454-5648
272. 冲击载荷损伤后C/C复合材料烧蚀性能的研究 , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2009,(3),37-40 ,DOI:10.3969/j.issn.1001-4381.2009.03.009, ISSN:1001-4381
273. 碳/碳复合材料导热性能的研究 , AAAS Press of Chinese Society of Aeronautics and Astronautics,2005,26(4),501-504 ,DOI:10.3321/j.issn:1000-6893.2005.04.025, ISSN:1000-6893
274. 闭孔碳微球泡沫材料制备工艺与性能研究 , Journal of Functional Materials,2005,36(12),1944-1946,1950 ,DOI:10.3321/j.issn:1001-9731.2005.12.039, ISSN:1001-9731
275. 热梯度CVI技术制备炭/炭复合材料 , Harbin Institute of Technology,2005,13(5),449-451 ,DOI:10.3969/j.issn.1005-0299.2005.05.001, ISSN:1005-0299
276. 碳/碳复合材料表面改性及其生物响应特性 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(4),60-66 ,DOI:10.3969/j.issn.1001-4381.2006.04.015, ISSN:1001-4381
277. 碳纤维增强水泥基复合材料屏蔽性能的研究 , Journal of Functional Materials,2006,37(8),1235-1238 ,DOI:10.3321/j.issn:1001-9731.2006.08.016, ISSN:1001-9731
278. 炭/炭复合材料热膨胀性能的研究 , Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China,2006,27(6),1-4 ,DOI:10.3969/j.issn.1009-6264.2006.06.001, ISSN:1009-6264
279. 热处理温度对中间相沥青基碳/碳复合材料力学性能的影响 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(1),15-18 ,DOI:10.3969/j.issn.1001-4381.2007.01.004, ISSN:1001-4381
280. 超声电沉积碳/碳复合材料磷灰石涂层的工艺优化 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(4),27-31 ,DOI:10.3969/j.issn.1001-4381.2007.04.007, ISSN:1001-4381
281. CVI treatment of short carbon fibers and their dispersion in CFRC , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(1),134-140 ,DOI:, ISSN:10003851
282. 纤维表面处理对C/C复合材料组织与性能的影响 , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2007,15(1),19-21,26 ,DOI:10.3969/j.issn.1005-0299.2007.01.005, ISSN:1005-0299
283. Process and properties of C/C composites by chemical liquid-vaporized infiltration , Xi'an Jiaotong University, West Xian Ning Road 28, Xi'an, 710049, China,2007,41(5),557-561 ,DOI:, ISSN:0253987X
284. 碳纤维增强水泥基复合材料的吸波性能研究 , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(5),756-759,763 ,DOI:10.3321/j.issn:1001-9731.2007.05.021, ISSN:1001-9731
285. 固化压力对一种纸基摩擦材料摩擦性能的影响 , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(4),118-122 ,DOI:10.3321/j.issn:1000-3851.2007.04.021, ISSN:1000-3851
286. 微观结构对中间相沥青基炭/炭复合材料力学性能的影响 , SCIENCE CHINA PRESS,2007,22(5),968-972 ,DOI:10.3321/j.issn:1000-324x.2007.05.038, ISSN:1000-324X
287. 氟化钠处理对炭/炭复合材料磷灰石生物活性涂层的影响 , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(6),89-94 ,DOI:10.3321/j.issn:1000-3851.2007.06.015, ISSN:1000-3851
288. 碳/碳复合材料表面的含氟磷灰石生物活性涂层 , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2007,21(6),570-576 ,DOI:10.3321/j.issn:1005-3093.2007.06.002, ISSN:1005-3093
289. Reflectivity of carbon-fiber-reinforced cement-based composites against electromagnetic waves , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi'an, 721014, China,2007,36(10),1702-1708 ,DOI:, ISSN:1002185X
290. 高温处理对炭/炭复合材料摩擦性能的影响 , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2007,15(5),606-609 ,DOI:10.3969/j.issn.1005-0299.2007.05.004, ISSN:1005-0299
291. Mechanical properties and microstructure of the joints between carbon-carbon composites and Ni based high temperature alloys , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi'an, 721014, China,2011,40(1),111-114 ,DOI:, ISSN:1002185X
292. 轴棒法编织C/C复合材料的热物理及烧蚀性能 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2011,34(1),113-118 ,DOI:10.3969/j.issn.1006-2793.2011.01.025, ISSN:1006-2793
293. C/C复合材料ZrC/SiC抗烧蚀涂层性能研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2011,34(1),105-108 ,DOI:10.3969/j.issn.1006-2793.2011.01.023, ISSN:1006-2793
294. 二甲苯热解制备C/C复合材料的组织结构及力学行为研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2011,34(2),241-246 ,DOI:10.3969/j.issn.1006-2793.2011.02.024, ISSN:1006-2793
295. 轴棒法编织三维四向C/C复合材料压缩及弯曲性能 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2011,34(2),256-260 ,DOI:10.3969/j.issn.1006-2793.2011.02.027, ISSN:1006-2793
296. 循环加载周期对二维C/C复合材料弯曲疲劳强度的影响 , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2011,28(2),100-104 ,DOI:, ISSN:1000-3851
297. 反向共沉淀法制备纳米Fe_3O_4及其粒径控制 , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2011,25(5),489-494 ,DOI:, ISSN:1005-3093
298. 碳纤维增强纸基摩擦材料磨损机理研究 , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2011,31(6),540-545 ,DOI:, ISSN:1004-0595
299. Joining of C/C composites and GH3128 Ni-based superalloy with Ni-Ti mixed powder as an interlayer , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi'an, 721014, China,2011,40(12),2088-2091 ,DOI:, ISSN:1002185X
300. 炭/炭复合材料C/SiC/MoSi2-SiC-Si抗氧化复合涂层 , ELSEVIER SCIENCE BV,2013,23(7),2118-2122 ,DOI:10.1016/S1003-6326(13)62705-3, ISSN:1003-6326
301. 3000°C氧-乙炔重复烧蚀后4D-炭/炭复合材料的剩余强度和热物理性能 , ELSEVIER SCIENCE BV,2013,23(6),1661-1667 ,DOI:10.1016/S1003-6326(13)62645-X, ISSN:1003-6326
302. Erratum: Microstructure and growth mechanism of ZrO2 nanorods network via oxyacetylene torch ablation (Materials Letters (2014) 123 (217-220)) , Elsevier,2014,131,116-117 ,DOI:10.1016/j.matlet.2014.05.075, ISSN:0167577X
303. Effect of microstructure on mechanical properties of mesophase pitch-based C/C composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2007,22(5),968-972 ,DOI:, ISSN:1000324X
304. Geometric simulation of holes in preform of four-step 3D braided composite , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2007,21(2),161-165 ,DOI:, ISSN:10053093
305. Investigation on ablation characteristics of C/C composites with ZrC/SiC coating , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2011,34(1),105-108 ,DOI:, ISSN:10062793
306. Preparation and ablation properties of SiC modified C/C composites , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2011,39(2),251-255 ,DOI:, ISSN:04545648
307. Thermophysical and ablative properties of axial carbon rod weaved 4D carbon/carbon composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2011,34(1),113-118 ,DOI:, ISSN:10062793
308. Graphite powder reinforced pyrocarbon, a new kind of C/C composite , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2007,22(1),12-16 ,DOI:, ISSN:10078827
309. Optimization of process parameters of calcium phosphate coating on C/C composites by sonoelectrodeposition technique , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(4),27-31 ,DOI:, ISSN:10014381
310. Effect of transition layer using mesophase pitch on mechanical properties of carbon/carbon composites , Chinese Journal of Materials Research,2006,20(4),381-385 ,DOI:, ISSN:10053093
311. Study on the shielding characteristics of carbon fiber reinforced cement composites , Journal of Functional Materials,2006,37(8),1235-1238 ,DOI:, ISSN:10019731
312. Study on microwave-absorbing properties of carbon-fiber-reinforced cement-based composites , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(5),756-759+763 ,DOI:, ISSN:10019731
313. Mechanism of defect formation and control of silicon carbide coating for carbon/carbon composites made by the pack cementation method , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2007,35(6),721-724 ,DOI:, ISSN:04545648
314. 纸基摩擦材料国内外研究进展 , 2010,,49-61 ,DOI:, ISSN:
315. Microstructure and oxidation resistance of SiC/W-Al-Si double-layer coatings for carbon-carbon composites , Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China,2011,32(7),17-20 ,DOI:, ISSN:10096264
316. Mechanical properties and microstructure of the joints between carbon-carbon composites and Ni based high temperature alloys , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi''an, 721014, China,2011,40(1),111-114 ,DOI:, ISSN:1002185X
317. Effects of heat treatment temperature on the friction performance of C/C composites , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2007,15(5),606-609 ,DOI:, ISSN:10050299
318. Research on anti-oxidation coatings for C/C composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2007,30(5),427-432 ,DOI:, ISSN:10062793
319. Study on microstructure uniformity of carbon/carbon composites prepared by chemical liquid-vaporized infiltration , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2007,30(5),437-441 ,DOI:, ISSN:10062793
320. Reflectivity of carbon-fiber-reinforced cement-based composites against electromagnetic waves , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi''an, 721014, China,2007,36(10),1702-1708 ,DOI:, ISSN:1002185X
321. W-Mo-Si/SiC oxidation protective coating for carbon/carbon composites , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2007,23(4),559-562 ,DOI:, ISSN:10050302
322. Growth process and mechanism of SiC whiskers by induction of carbon fiber , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2007,35(5),643-647 ,DOI:, ISSN:04545648
323. Process and properties of C/C composites by chemical liquid-vaporized infiltration , Xi''an Jiaotong University, West Xian Ning Road 28, Xi''an, 710049, China,2007,41(5),557-561 ,DOI:, ISSN:0253987X
324. 碳/碳复合材料表面ZrC涂层结构和烧蚀性能研究 , 2013,,107-112 ,DOI:, ISSN:
325. SiC纳米线改性界面层对C/C复合材料与LAS连接性能的影响 , 2013,,166-170 ,DOI:, ISSN:
326. 增强纤维对纸基摩擦材料性能的影响研究 , 2009,,316-320 ,DOI:, ISSN:
327. 炭复合材料C/SiC/Si-Mo高温抗氧化复合涂层研究 , 2009,,371-375 ,DOI:, ISSN:
328. 连接温度对C/C和GH3128连接接头性能和结构的影响 , 2009,,542-545 ,DOI:, ISSN:
329. 固体火箭发动机条件下炭/炭复合材料喉衬的烧蚀行为研究 , 2009,,546-550 ,DOI:, ISSN:
330. 碳纤维增强水泥基复合材料(CFRC)的电磁性能 , 2009,,29-42 ,DOI:, ISSN:
331. 3DC/C复合材料的弯曲性能及断裂特征 , 2005,,377-380 ,DOI:, ISSN:
332. 炭/炭复合材料的碳化钨接头及其电性能研究 , 2005,,373-376 ,DOI:, ISSN:
333. 焦炭种类对沥青基炭复合材料力学各向异性系数的影响 , 2005,,359-361 ,DOI:, ISSN:
334. Effect of carbonization pressure on microstructure and morphology of pitch derived carbon , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2006,27(5),969-972 ,DOI:, ISSN:10006893
335. Thermal expansion property of carbon/carbon composite , Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China,2006,27(6),1-4 ,DOI:, ISSN:10096264
336. Joining of C/C composites and GH3128 Ni-based superalloy with Ni-Ti mixed powder as an interlayer , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi''an, 721014, China,2011,40(12),2088-2091 ,DOI:, ISSN:1002185X
337. Wear mechanism of carbon fiber reinforced paper-based friction material , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2011,31(6),540-545 ,DOI:, ISSN:10040595
338. Prefabrication of SiC coating to protect C/C composites with carbonizing rice hull , Beijing Institute of Aeronautical Materials (BIAM), Beijing, 100095, China,2007,(6),11-14 ,DOI:, ISSN:10014381
339. 应力比对2.5D C/C复合材料弯-弯疲劳行为的影响 , 2015,34(1),27-31 ,DOI:10.14078/j.cnki.1001-3741.2015.01.007, ISSN:1001-3741
340. Effects of NaF treatment on the bioactive apatite coating for C/C composites , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(6),89-94 ,DOI:, ISSN:10003851
341. Dispersion of carbon fibers and conductivity of carbon-fiber-reinforced cement-based composites , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(10),1641-1644 ,DOI:, ISSN:10019731
342. FHA coating for C/C composites prepared by sonoelectrodeposition and treatment of NaF , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(8),1320-1323+1326 ,DOI:, ISSN:10019731
343. SiC coating prepared by a two-step technique of pack cementation and CVD on carbon/carbon composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2007,22(4),737-741 ,DOI:, ISSN:1000324X
344. Influence of curing pressure on the friction performance of a kind of paper based friction material , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(4),118-122 ,DOI:, ISSN:10003851
345. Effect of fiber surface treatment on the microstructure and mechanical properties of mesophase pitch-based C/C composites , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2007,15(1),19-21+26 ,DOI:, ISSN:10050299
346. CVI treatment of short carbon fibers and their dispersion in CFRC , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(1),134-140 ,DOI:, ISSN:10003851
347. Synthesis and size control of the nano-Fe3O4 particles synthesized by a reverse coprecipitation method , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2011,25(5),489-494 ,DOI:, ISSN:10053093
348. Effect of cycles on flexural fatigue strength for 2D C/C composites , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2011,28(2),100-104 ,DOI:, ISSN:10003851
349. Compression and bending properties of 4D C/C composite insert by weaved with carbon fiber and axial carbon rod , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2011,34(2),256-260 ,DOI:, ISSN:10062793
350. Microstructure and mechanical behavior of carbon/carbon composites prepared from xylene pyrolysis , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2011,34(2),241-246 ,DOI:, ISSN:10062793
351. Research on microstructure and oxidation resistance of SiC/Al-Si coating for carbon-carbon composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(4),43-46 ,DOI:, ISSN:10014381
352. Effects of heat treatment temperature on mechanical properties of mesophase pitch-based C/C composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(1),15-18 ,DOI:, ISSN:10014381
353. Microstructures and mechanical properties of carbon/carbon composites prepared by impulse forced flow thermal gradient chemical vapor infiltration , Editorial Board of New Carbon Materials,2006,21(2),132-138 ,DOI:10.1016/j.neulet.2005.11.025, ISSN:10078827
354. Mechanical properties of short carbon fiber reinforced pitch-based carbon/carbon composites , Editorial Board of New Carbon Materials,2006,21(1),36-42 ,DOI:, ISSN:10078827
355. 羰基铁粉-碳纤维水泥基复合材料的吸波性能 , 2010,,69-74 ,DOI:, ISSN:
356. Z向缝合增强C/C复合材料在低能冲击下的损伤研究 , 2003,,288-290 ,DOI:, ISSN:
357. Microstructure and mechanical properties of C/C-ZrC composites , Science Press,2015,30(5),459-466 ,DOI:10.15541/jim20140455, ISSN:1000324X
358. An approach to synthesis isolated carbon nanotubes with bamboo-like structures , 2007, ,DOI:, ISSN:
359. 催化裂解简单合成离散的短纳米碳管 , 2006,,2348-2350 ,DOI:, ISSN:
360. 纸基摩擦材料的绿色制备工艺与摩擦磨损性能研究 , 2003,,12-16 ,DOI:, ISSN:
361. 炭化压力对中间相沥青过渡层炭/炭复合材料组织与性能的影响 , 2007,,39-45 ,DOI:, ISSN:
362. 炭/炭复合材料MoSi2-SiC-Si/SiC/玻璃复合涂层高温抗冲刷性能研究 , 2007,,463-467 ,DOI:, ISSN:
363. 溴插层对C/C复合材料致密化效率的影响 , 2007,,450-453 ,DOI:, ISSN:
364. 化学液相气化沉积制备炭/炭复合材料的影响因素分析 , 2007,,425-430 ,DOI:, ISSN:
365. 均匀化技术对短炭纤维增强沥青碳基C/C复合材料性能的影响 , 2007,,367-372 ,DOI:, ISSN:
366. 焦炭颗粒增强沥青基炭复合材料的组织结构 , 2008,,92-97 ,DOI:, ISSN:
367. 炭/炭复合材料高温防氧化SiC/SiC-MoSi2多层复合涂层研究 , 2008,,223-229 ,DOI:, ISSN:
368. C/C复合材料正压CVI工艺的研究探索 , 1999,,31-34 ,DOI:, ISSN:
369. 2D碳/碳复合材料CVI工艺的数值模拟与分析 , 1998,,182~186 ,DOI:, ISSN:
370. 难熔金属氧化物对C/C复合材料SiC涂层组织结构的影响 , 0,,453-456 ,DOI:, ISSN:
371. 碳/碳复合材料研究应用现状及思考 , 2001,,24-28 ,DOI:, ISSN:
372. 热梯度CVI工艺制备碳/碳复合刹车材料 , 2004,,780-783 ,DOI:, ISSN:
373. 炭/炭复合材料CVI工艺的热解炭沉积机理研究 , 2003,,44-48 ,DOI:, ISSN:
374. 不连续碳纤维增强C/C复合材料的研究现状 , 2003,,280-283 ,DOI:, ISSN:
375. 钨酚醛树脂连接炭/炭复合材料的工艺研究 , 2004,,1-4 ,DOI:, ISSN:
376. 一种新型炭材料——石墨颗粒增强热解炭基复合材料 , 2004,,12-15 ,DOI:, ISSN:
377. C/C复合材料表面SiC-MoSi2/ZrO2-MoSi2防氧化涂层研究 , 2012,,28-34 ,DOI:, ISSN:
378. 乙醇与甲烷混合前驱体制备炭/炭复合材料 , 2012,,93-99 ,DOI:, ISSN:
379. C/C-碳泡沫组合材料的制备与性能研究 , 2011,,415-420 ,DOI:, ISSN:
380. 沉积温度对各向同性热解炭微观结构及力学性能的影响 , 2011,,430-435 ,DOI:, ISSN:
381. 沉积温度对C/C复合材料致密化的影响 , 2011,,62-70 ,DOI:, ISSN:
382. 碳化硅纳米线基本力学性能的细观力学估算 , 2009,,138-138 ,DOI:, ISSN:
383. 石墨粒度对纸基摩擦材料摩擦磨损性能的影响 , 2011,,63-68 ,DOI:, ISSN:
384. 热处理温度对炭/炭复合材料性能的影响 , 2011,,237-242 ,DOI:, ISSN:
385. 炭/炭复合材料CVI工艺的热解炭沉积机理研究 , 2011,,243-249 ,DOI:, ISSN:
386. C/C复合材料比热容和热扩散率的研究 , 2011,,250-253 ,DOI:, ISSN:
387. Electromagnetic interference of ferrocene-doped carbon fiber-reinforced cement composites , Trans Tech Publications, P.O. Box 1254, Clausthal-Zellerfeld, D-38670, Germany,2011,261-263,638-641 ,DOI:10.4028/www.scientific.net/AMR.261-263.638, ISSN:9783037851418
388. Effect of the fabrication process on the properties of pitch-based carbon-carbon composites , International Committee on Composite Materials, Vancouver, BC, V6T 1Z4, Canada,2009, ,DOI:, ISSN:
389. Mechanical property evaluation of C/C composite material grids for electron cyclotron resonance thruster , Journal of Propulsion Technology, P.O. Box 7208-26, Beijing, 100074, China,2007,28(6),692-696 ,DOI:, ISSN:10014055
390. 应力比对2.5D C/C复合材料弯-弯疲劳行为的影响 , 2014,,53-61 ,DOI:, ISSN:
391. Template-free Hydrothermal Synthesis of Copper Phthalocyanine Nanobelts , CHEMICAL SOC JAPAN,2015,44(5),592-594 ,DOI:10.1246/cl.150016, ISSN:0366-7022
392. Numerical simulation of chemical vapor infiltration for 2D C/C composites , China Spaceflight Soc, China,1999,20(4),104-107 ,DOI:, ISSN:10001328
393. One-Step Solvothermal Synthesis of Tetranitro-Cobalt Phthalocyanine/Reduced Graphene Oxide Composite , WORLD SCIENTIFIC PUBL CO PTE LTD,2015,10(3) ,DOI:10.1142/S1793292015500459, ISSN:1793-2920
394. Novel thermal gradient chemical vapor infiltration process for carbon-carbon composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2007,22(3),247-252 ,DOI:10.1016/S1872-5805(07)60020-1, ISSN:
395. Microstructure and fabrication of C/C composites at super-short gas residence time , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2009,(9),33-37 ,DOI:, ISSN:10014381
396. Effect of Si/Mo ratio on microstructure and high-temperature antioxidation property of SiC-MoSi2 coating for carbon/carbon composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2008,31(3),283-287 ,DOI:, ISSN:10062793
397. Preparation of bromine intercalated pyrolytic carbon , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2008,23(2),185-188 ,DOI:, ISSN:10078827
398. 造粒粉体对SiC陶瓷力学性能及微观组织的影响 , 2015,(3),250-255 ,DOI:10.13957/j.cnki.tcxb.2015.03.007, ISSN:1000-2278
399. Pyrocarbon transition layer and microstructure of mesophase pitch based carbon/carbon fiber composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2010,25(4),297-302 ,DOI:, ISSN:10078827
400. Study on antioxidant mechanism of refractory metallic disilicide coating for carbon/carbon composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2010,33(2),218-221 ,DOI:, ISSN:10062793
401. A SiC-HfSi2 anti-ablation compound coating of carbon/carbon composite , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2010,38(2),352-356 ,DOI:, ISSN:04545648
402. The thermal expansion behavior of 3D C/C composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2010,25(1),60-64 ,DOI:, ISSN:10078827
403. Oxidation behavior of C/C composites with SiC coating , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2010,33(1),91-94 ,DOI:, ISSN:10062793
404. Advancement of high-temperature oxidation resistant ceramic coatings for carbon/carbon composites , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2010,(8),86-91 ,DOI:, ISSN:10014381
405. Connection between carbon-carbon composites and LAS ceramic with YAST glass-ceramic reinforced by CNTs , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2010,33(4),459-462 ,DOI:, ISSN:10062793
406. Research on preparation and property of borosilicate glass coating for C/C composites , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2010,(7),78-81+86 ,DOI:, ISSN:10014381
407. Yttrium silicate coatings for SiC coated C/C composites prepared by atmospheric plasma spraying , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2010,25(3),187-191 ,DOI:, ISSN:10078827
408. Reflection properties against electromagnetic waves of chopped carbon fiber reinforced cement mortar , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2010,41(SUPPL. 1),89-93 ,DOI:, ISSN:10019731
409. Research progress on high temperature oxidation protective silicon-based ceramic coatings for carbon fiber reinforced carbon composites , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2010,38(5),991-996 ,DOI:, ISSN:04545648
410. Microstructure of pitch-based C/C composites fabricated by HPIC technology , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2008,16(6),755-758 ,DOI:, ISSN:10050299
411. Research on thermal conduction and mechanical properties for carbon foam , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(6),1171-1174 ,DOI:10.3724/SP.J.1077.2008.01171, ISSN:1000324X
412. Fabrication and reinforcing mechanism: In-situ grown carbon nanotube reinforced carbon/carbon composites with high interlaminar shear strength , Trans Tech Publications Ltd, Kreuzstrasse 10, Zurich-Durnten, CH-8635, Switzerland,2013,748,74-78 ,DOI:10.4028/www.scientific.net/AMR.748.74, ISSN:9783037857526
413. Synthesis of Low-dimensional Nano-structural GaN , Northwest Institute for Nonferrous Metal Research,2002,31(5),324 ,DOI:, ISSN:1002185X
414. Friction performance of paper type friction material in limited lubricating condition , Science Press,2005,(3),40-43 ,DOI:, ISSN:02540150
415. Effect of graphite content on the friction and wear performance of paper-based friction materials , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2007,27(5),451-455 ,DOI:, ISSN:10040595
416. Study on the oxidation mechanism of the coated C/C composites , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(8),1327-1330 ,DOI:, ISSN:10019731
417. HfB2 prepared by sol-gel method and its oxidation behavior , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi''an, 721014, China,2013,42(12),2594-2597 ,DOI:, ISSN:1002185X
418. SiC-Si-ZrSiO4 multiphase oxidation protective coating for carbon/carbon composites , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2008,24(6),941-944 ,DOI:, ISSN:10050302
419. Effects of current density on structure and morphology of brushite by sonoelectrodeposition technique , Northwest Institute for Nonferrous Metal Research, Xian, China,2003,32(11),923-926 ,DOI:, ISSN:1002185X
420. Wave-absorbing properties of carbonyl iron powder/carbon fiber reinforced cement-based composites , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2011,39(1),69-74 ,DOI:, ISSN:04545648
421. Ultra-High-Temperature Ceramic HfB2-SiC Coating for Oxidation Protection of SiC-Coated Carbon/Carbon Composites , WILEY-BLACKWELL,2015,12(3),560-567 ,DOI:10.1111/ijac.12241, ISSN:1546-542X
422. PTLP bonding C/C composites to super-alloy GH3044 with Ni/Ti interlayer , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2012,35(3),414-418 ,DOI:, ISSN:10062793
423. Effect of hafnium carbide content on the ablative performance of carbon/carbon composites as rocket throats , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2012,27(4),311-314 ,DOI:, ISSN:10078827
424. Preparation of montmorillonite-modified carbon foams , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2014,29(2),143-148 ,DOI:, ISSN:10078827
425. Effect of the molding pressure on properties of pitch-based carbon composites reinforced with granular cokes , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2009,32(5),559-564 ,DOI:, ISSN:10062793
426. Microstructure and antioxidation properties of SiC-MoSi2/SiC coating for C/C composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2008,31(6),638-641 ,DOI:, ISSN:10062793
427. Ablation performances of the HfC modified carbon/carbon composite integrated throat , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(6),1155-1158 ,DOI:10.3724/SP.J.1077.2008.01155, ISSN:1000324X
428. Preparation and property characterization of C/SiC composite thruster , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2008,31(4),393-396+411 ,DOI:, ISSN:10062793
429. Curing characteristics and kinetic analysis of furfural acetone resin used as carbon/carbon composites precursor , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2012,35(1),123-126+132 ,DOI:, ISSN:10062793
430. T-S fuzzy system for isothermal CVI process of C/C Composites , China Spaceflight Society, Beijing, China,2004,25(1),119-122 ,DOI:, ISSN:10001328
431. Numerical simulation of thermal-gradient CVI process for C/C composite , Beijing University of Aeronautics and Astronautics (BUAA),2000,17(4),84-87 ,DOI:, ISSN:10003851
432. Neural network simulation on effect of burning rate of modified carbon/carbon composites , Xi''an Jiaotong University,2003,37(3),249-251+330 ,DOI:, ISSN:0253987X
433. Friction performance of C/C composites by rapid densification with different preforms , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2008,31(4),403-407 ,DOI:, ISSN:10062793
434. Analysis of tangential deformation of metal in tube spinning , NPU, Xi''an, China,1998,16(4),627-631 ,DOI:, ISSN:10002758
435. Prediction of dimensional precision of inner diameter in spun parts , 1998,(5),11-13 ,DOI:, ISSN:10008756
436. Numerical simulation of residual stress of spun cylindrical shapes , 1998,5(3),57-60 ,DOI:, ISSN:10072012
437. Influence of process parameters on residual stress distribution in backward tube spinning , 1997,22(4),23-25, 36 ,DOI:, ISSN:10003940
438. Microstructure and mechanical properties of C/C composites with a mesophase pitch transition layer , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(3),486-490 ,DOI:10.3724/SP.J.1077.2008.00486, ISSN:1000324X
439. Study on the electromagnetic interference of CFRC composites by reflectivity , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2008,24(2),265-271 ,DOI:, ISSN:10050302
440. Effect of surface roughness of carbon/carbon composites on osteoblasts growth behaviour , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(2),341-345 ,DOI:10.3724/SP.J.1077.2008.00341, ISSN:1000324X
441. Preparation and properties of carbon fiber needling preform reinforced silicon carbide composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(2),223-228 ,DOI:10.3724/SP.J.1077.2008.00223, ISSN:1000324X
442. Effect of impact damage on ablative performances of the carbon/carbon composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(2),219-222 ,DOI:10.3724/SP.J.1077.2008.00219, ISSN:1000324X
443. Investigation of the multi-coating for high temperature and long life oxidation protection of C/C composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(2),213-218 ,DOI:10.3724/SP.J.1077.2008.00213, ISSN:1000324X
444. Friction and wear performance of carbon/carbon composites by CLVI process under wet conditions , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,28(1),50-55 ,DOI:, ISSN:10040595
445. Bioactive hydroxyapatite coating on carbon/carbon composite prepared by sonoelectrodeposition and alkaline-heat treatment , Rare Metals Materials and Engineering Press, Xi''an, China,2005,34(9),1489-1492 ,DOI:, ISSN:1002185X
446. C/C复合材料航空电刷的制备 , 2004,,47-50 ,DOI:, ISSN:
447. C/C复合材料SiC-WSi2/MoSi2复合涂层的抗氧化性能研究 , 2008,,85-91 ,DOI:, ISSN:
448. SiC/Si-W-Mo coating for protection of C/C composites at 1873 K , University of Science and Technology Beijing, 30 Xueyuan Lu, Beijing, 100083, China,2008,15(6),822-826 ,DOI:10.1016/S1005-8850(08)60294-7, ISSN:10058850
449. Flexural behavior of 2D carbon-carbon composites fabricated by pressure gradient CVI , Editorial Board of New Carbon Materials,2004,19(4),289-292 ,DOI:, ISSN:10078827
450. Influence of heat treatment on oxidation properties of C/C composites fabricated by high pressure impregnation carbonization , Chinese Academy of Sciences,2004,17(4),426-430 ,DOI:, ISSN:10067191
451. Influence of graphitization on oxidation resistance of carbon/carbon composites prepared by high pressure impregnation and carbonization , Chinese Ceramic Society,2004,32(12),1515-1519 ,DOI:, ISSN:04545648
452. Microstructural characteristics of short carbon fiber reinforced pitch-based carbon/carbon composites , Editorial Board of New Carbon Materials,2004,19(2),119-123 ,DOI:, ISSN:10078827
453. Advance in research on tribological behavior and mechanism of carbon/carbon composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2004,(12),59-62 ,DOI:, ISSN:10014381
454. Research on chemical vapor infiltration of pyrolytic carbon for carbon/carbon composites , Rare Metals Materials and Engineering Press, Xi''an, China,2004,33(SUPPL.),44-48 ,DOI:, ISSN:1002185X
455. Modeling of isothermal CVI process of C/C composites by fuzzy neural network , Rare Metals Materials and Engineering Press, Xi''an, China,2004,33(10),1037-1040 ,DOI:, ISSN:1002185X
456. Progressing in the study on mechanical properties of the 3D braided composites , Beijing Institute of Aeronautical Materials (BIAM),2004,(2),44-48 ,DOI:, ISSN:10014381
457. Fuzzy system model for isothermal chemical vapor infiltration process of carbon/carbon composites , Chinese Ceramic Society,2003,31(7),629-634 ,DOI:, ISSN:04545648
458. Mamdani fuzzy system for isothermal CVI process of C/C composites , Chinese Journal of Materials Research,2003,17(4),375-379 ,DOI:, ISSN:10053093
459. Microstructure and mechanical properties of C/C composite bolts , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2012,35(2),248-252 ,DOI:, ISSN:10062793
460. Effect of different oxide additives on the properties of a SiC coating on carbon/carbon composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2009,24(1),45-49 ,DOI:, ISSN:10078827
461. Effect of surface treatments of short carbon fibers on the properties of pitch-based C/C composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2009,24(1),89-92 ,DOI:, ISSN:10078827
462. Joining of surface modified carbon/carbon composites and LAS glass ceramic , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2009,30(2),380-384 ,DOI:, ISSN:10006893
463. Preparation and performance of pre-coated carbon layer for carbon/carbon composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2009,24(1),125-128 ,DOI:10.3724/SP.J.1077.2009.00125, ISSN:1000324X
464. Investigation on microstructure and oxidation resistance of SiC/mullite-Si-Al2O3 coating for carbon/carbon composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2009,32(2),226-229 ,DOI:, ISSN:10062793
465. Ablation behaviors of Carbon/Carbon composites after impact damage , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2009,(3),37-40 ,DOI:, ISSN:10014381
466. Influence of homogenization method on fiber homogeneous effect and properties of C/C composite , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2009,32(1),95-99 ,DOI:, ISSN:10062793
467. Effects of fiber volume fraction and thermal treatment on the properties of C/C composites , Chinese Journal of Materials Research,2005,19(3),293-298 ,DOI:, ISSN:10053093
468. SiC-HfSi2-TaSi2 high temperature anti-ablation compound coating on carbon/carbon composites , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2009,37(5),804-807 ,DOI:, ISSN:04545648
469. Preparation and anti-oxidation property of SiC/SiC-MoSi2 coating on C/C composite , Chinese Academy of Sciences, 72 Wenhua Road, Shenyang, 110015, China,2009,45(4),503-506 ,DOI:, ISSN:04121961
470. Preparation for 2D-C/C composites with pure RL textures and its characteristic , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2009,23(2),138-142 ,DOI:, ISSN:10053093
471. SiC/Si-Al2O3-mullite oxidation protective coating for C/C composites prepared by in-situ formation method , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2009,30(3),551-556 ,DOI:, ISSN:10006893
472. The infiltration process and texture transition of 2D C/C composites , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2009,25(1),109-114 ,DOI:, ISSN:10050302
473. Influence of thermal shock on the mechanical behavior of Si-SiC coated carbon/carbon composites , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2009,25(2),251-253 ,DOI:, ISSN:10050302
474. Effect of molybdenum and tungsten on reactive joint of carbon-carbon composites , Rare Metals Materials and Engineering Press, Xi''an, China,2005,34(SUPPL. 2),367 ,DOI:, ISSN:1002185X
475. Preparation and oxidation kinetics of SiC/ZrO2-SiO2 oxidation protective coating for carbon-carbon composites , Rare Metals Materials and Engineering Press, Xi''an, China,2005,34(SUPPL. 2),328 ,DOI:, ISSN:1002185X
476. Fabrication of anodic alumina membrane , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2005,(5),56-59+64 ,DOI:, ISSN:10014381
477. Si-SiC oxidation protective coating for carbon/carbon composites , Rare Metals Materials and Engineering Press, Xi''an, China,2005,34(SUPPL. 2),263-264 ,DOI:, ISSN:1002185X
478. Effect of granular reinforcements on the properties of pitch-based carbon composites , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2008,23(1),51-57 ,DOI:, ISSN:10078827
479. Surface thermal treatment of carbon fibers and electromagnetic shielding of carbon fiber/cement composites , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2008,36(10),1348-1355 ,DOI:, ISSN:04545648
480. Mechanical properties of C/SiC/Si-Mo-Cr multilayer coated carbon/carbon composites , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,23(4),725-728 ,DOI:10.3724/SP.J.1077.2008.00725, ISSN:1000324X
481. Influence of in-situ grown carbon nanotubes on carbon fiber on the flexural properties of C/C composites , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2013,30(6),7-13 ,DOI:, ISSN:10003851
482. Densification of C/C composites using film boiling chemical vapor infiltration with two heaters , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2013,28(6),442-447 ,DOI:, ISSN:10078827
483. Tribological properties of polytetrafluoroethylene (PTFE) composite coating on carbon-carbon composites , Xi''an Jiaotong University,2006,40(1),72-74+105 ,DOI:, ISSN:0253987X
484. Fracture characteristics of carbon/carbon composites prepared by mix technics , Rare Metals Materials and Engineering Press, Xi''an, China,2006,35(SUPPL. 2),245-248 ,DOI:, ISSN:1002185X
485. Research on carbon film doped with chromium on the carbon-carbon composites with SiC interlayer , Rare Metals Materials and Engineering Press, Xi''an, China,2006,35(8),1204-1207 ,DOI:, ISSN:1002185X
486. Effects of flexural fatigue loading on thermal expansion behavior of 2D-C/C composites , Journal of Solid Rocket Technology, P.O. Box 120, Xi''an, 710025, China,2012,35(5),665-669 ,DOI:, ISSN:10062793
487. Deposition model and microstructure of low temperature pyrocarbon produced by chemical vapor deposition , Editorial Board of New Carbon Materials, P.O.Box 165, Taiyuan, 030001, China,2012,27(2),81-86 ,DOI:, ISSN:10078827
488. Effects of heat treatment temperature on the properties of C/C composites , Editorial Office of Transactions of Materials and Heat Treatment,2005,26(1),1-4 ,DOI:, ISSN:10096264
489. Effect of depositing position on microstructure of SiC coating by chemical vapor deposition , Xi''an Jiaotong University,2005,39(1),49-52 ,DOI:, ISSN:0253987X
490. Effect of the average particle size of granular pitch coke on properties of pitch-based granular coke reinforced carbon composites , Editorial Board of New Carbon Materials,2005,20(3),235-239 ,DOI:, ISSN:10078827
491. Effects of heat treatment temperature on the joining properties of C/C composites using molybdenum phenolic resin , Editorial Office of Transactions of Materials and Heat Treatment,2005,26(4),5-7 ,DOI:, ISSN:10096264
492. Research on the thermal conductivity of C/C composites , AAAS Press of Chinese Society of Aeronautics and Astronautics,2005,26(4),501-504 ,DOI:, ISSN:10006893
493. Thermal gradient CVI for fabrication of carbon/carbon composites tubes , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(SUPPL.),345-348 ,DOI:, ISSN:10014381
494. Numerical simulation of temperature field in thermal gradient CVI process for carbon/carbon composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(SUPPL.),326-328+333 ,DOI:, ISSN:10014381
495. Microstructure and mechanical properties of mesophase pitch-based C/C composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(5),21-24 ,DOI:, ISSN:10014381
496. Surface modification technologies and biological response properties of bioactive coatings on carbon/carbon composites , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(4),60-66 ,DOI:, ISSN:10014381
497. Growth mechanism of the calcium phosphate coatings on C/C composites by sonoelectrodeposition technique , Rare Metals Materials and Engineering Press, Xi''an, China,2006,35(7),1096-1100 ,DOI:, ISSN:1002185X
498. Ablation behavior of HfC modified carbon/carbon composites , Rare Metals Materials and Engineering Press, Xi''an, China,2006,35(SUPPL. 2),365-368 ,DOI:, ISSN:1002185X
499. Progress on the oxidation protective coating of carbon-carbon composites , Editorial Board of New Carbon Materials,2005,20(4),373-379 ,DOI:, ISSN:10078827
500. Study on preparation of closed-celled microspheric carbon foams , Journal of Functional Materials,2005,36(12),1944-1946+1950 ,DOI:, ISSN:10019731
501. High Enhanced Efficiency and Mechanism of Ultra-Long SiC Nanowires in Composites , WILEY-V C H VERLAG GMBH,2015,17(4),539-544 ,DOI:10.1002/adem.201400194, ISSN:1438-1656
502. 碳/碳复合材料高温抗氧化涂层研究新进展 , 2006,,15-21 ,DOI:, ISSN:
503. Catalytic Activity for Oxygen Reduction of Dual Catalysts System Based on Tetranitro-Metal Phthalocyanine and Nano-Manganese Dioxide , TAYLOR & FRANCIS INC,2015,45(12),1813-1818 ,DOI:10.1080/15533174.2013.867880, ISSN:1553-3174
504. 弯曲载荷下纯净光滑层热解炭基2D-C/C复合材料的断裂机制 , ELSEVIER SCIENCE BV,2013,23(7),2141-2146 ,DOI:10.1016/S1003-6326(13)62709-0, ISSN:1003-6326
505. 六棱柱状SiC纳米线的制备与表征 , 2005,,577-582 ,DOI:, ISSN:
506. 炭/炭复合材料磷酸盐涂层的抗氧化性能研究 , 2004,,95-100 ,DOI:, ISSN:
507. 热梯度化学气相沉积制备炭/炭复合材料制件 , 2004,,120-123 ,DOI:, ISSN:
508. 专家系统在复合材料研究中的应用 , 2002,,1025-1029 ,DOI:, ISSN:
509. 声电沉积制备碳/碳复合材料生物活性透钙磷石涂层研究 , 2002,,60-64 ,DOI:, ISSN:
510. In-situ Preparation of TiB2-TiB-Ti Functionally Graded Materials by Improved Sintering Process , JOURNAL WUHAN UNIV TECHNOLOGY,2015,30(4),710-714 ,DOI:10.1007/s11595-015-1216-4, ISSN:1000-2413
511. 难熔金属氧化物对C/C复合材料SiC涂层组织结构的影响 , 2004,,453-456 ,DOI:, ISSN:
512. C/C复合材料SiC—WSi2/MoSi2复合涂层的抗氧化性能研究 , 2008,,85-91 ,DOI:, ISSN:
513. 炭/炭复合材料复合涂层高温燃气环境下的抗冲刷性能研究 , 2008,,230-237 ,DOI:, ISSN:
514. Rectangle preform simulation for 3-D braided composites , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2006,27(5),985-988 ,DOI:, ISSN:10006893
515. B<,2>O<,3>-SiC自润滑涂层炭/炭复合材料的性能研究 , 2005,,429-432 ,DOI:, ISSN:
516. 二维炭/炭复合材料微氧化机理及氧化模型研究 , 2005,,346-349 ,DOI:, ISSN:
517. Fluorine-containing hydroxyapatite bioactive coating on the surface of C/C composites , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2007,21(6),570-576 ,DOI:, ISSN:10053093
518. Investigation on microstructure and oxidation resistance of Cr-Al-Si coating for carbon/carbon composites by plasma spraying , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(5),109-112 ,DOI:, ISSN:10003851
519. 炭/炭复合材料防氧化SiC纳米线增韧MoSi2-SiC涂层研究 , 2009,,551-555 ,DOI:, ISSN:
520. Mechanical properties and microstructure of the joints between carbon-carbon composites and Ni based high temperature alloys , Rare Metals Materials and Engineering Press, P.O. Box 51, Xi''an, 721014, China,2011,40(1),111-114 ,DOI:, ISSN:
521. Catalytic chemical vapor infiltration of carbon nanofilament network reinforced carbon/carbon composites: Catalytic effect on the densification behavior and matrix microstructure , International Astronautical Federation, IAF,2013,8,5865-5896 ,DOI:, ISSN:9781629939094
522. 炭/炭复合材料导热性能的研究 , 2011,,254-258 ,DOI:, ISSN:
523. Neural network modeling method for silicon carbide chemical vapor deposition process , Chinese Ceramic Society, China,2000,28(1),25-29 ,DOI:, ISSN:04545648
524. Study on the green preparation process and friction performance of paper-type friction material , Science Press,2004,24(2),172-176 ,DOI:, ISSN:10040595
525. Effect of chemical vapor infiltration treatment on the wave-absorbing performance of carbon fiber/cement composites , University of Science and Technology Beijing, 30 Xueyuan Lu, Beijing, 100083, China,2008,15(6),808-815 ,DOI:10.1016/S1005-8850(08)60292-3, ISSN:10058850
526. Study of the SiC-TaSi2/MoSi2 multilayer oxidation protective coating for carbon/carbon composite , Chinese Academy of Sciences, 72 Wenhua Road, Shenyang, 110015, China,2008,44(3),331-335 ,DOI:, ISSN:04121961
527. Si-Al-Ir oxidation resistant coating for carbon/carbon composites by slurry dipping , Chinese Society of Metals, 72 Wenhua Road, Shenyang, 110015, China,2009,25(3),344-346 ,DOI:, ISSN:10050302
528. Research on thermal gradient CVI process for preparing carbon/carbon composites , Harbin Institute of Technology,2005,13(5),449-451 ,DOI:, ISSN:10050299
529. SiC/Cr-Al-Si/glass multilayer oxidation resistant coating for carbon/carbon composites , MANEY PUBLISHING,2011,27(5),340-344 ,DOI:10.1179/174329409X409431, ISSN:0267-0844
530. Research on chemical vapor infiltration of pyrolytic carbon for carbon/carbon composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2004,33(6),44-48 ,DOI:, ISSN:1002-185X
531. Microstructure of the pyrocarbon matrix prepared by the CLVI process , ELSEVIER SCIENCE SA,2004,369(1-2),245-249 ,DOI:10.1016/j.msea.2003.11.025, ISSN:0921-5093
532. A new SiC/yttrium silicate/glass multi-layer oxidation protective coating for carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2004,42(11),2356-2359 ,DOI:10.1016/j.carbon.2004.05.005, ISSN:0008-6223
533. Damage to thickness-reinforced C/C laminates by low-energy impact , PERGAMON-ELSEVIER SCIENCE LTD,2004,42(14),3033-3036 ,DOI:10.1016/j.carbon.2004.07.007, ISSN:0008-6223
534. Micro-pleating in carbon-carbon composites under a cyclic load , SCIENCE CHINA PRESS,2003,46(4),337-342 ,DOI:10.1360/02ye0316, ISSN:1006-9321
535. Synthesis of the various morphologies GaN one-dimensional nanomaterials , KLUWER ACADEMIC PUBL,2003,22(11),831-833 ,DOI:10.1023/A:1023968310697, ISSN:0261-8028
536. Optimizing parameters of CVI process for manufacturing carbon-carbon composites by genetic algorithms , ELSEVIER SCIENCE BV,2003,57(16-17),2366-2370 ,DOI:10.1016/S0167-577X(02)01236-3, ISSN:0167-577X
537. Modeling of CVI process in fabrication of carbon/carbon composites by an artificial neural network , SCIENCE CHINA PRESS,2003,46(2),173-181 ,DOI:10.1360/03ye9019, ISSN:1006-9321
538. SiC nanowire networks , ELSEVIER SCIENCE SA,2003,352(1-2),279-282 ,DOI:10.1016/S0925-8338(02)01111-8, ISSN:0925-8388
539. Large-scale synthesis of crystalline beta-SiC nanowires , SPRINGER,2003,76(4),637-640 ,DOI:10.1007/s00339-002-1961-z, ISSN:0947-8396
540. beta-Ga2O3 nanowires on unpatterned and patterned MgO single crystal substrates , ELSEVIER SCIENCE SA,2002,345(1-2),275-279 ,DOI:10.1016/S0925-8388(02)00414-0, ISSN:0925-8388
541. Numerical design of the die land for shape extrusion , ELSEVIER SCIENCE SA,2000,101(1-3),81-84 ,DOI:10.1016/S0924-0136(00)00437-4, ISSN:0924-0136
542. Numerical simulation of isothermal chemical vapor infiltration process in fabrication of carbon-carbon composites by finite element method , SCIENCE PRESS,2000,43(1),77-85 ,DOI:10.1007/BF02917140, ISSN:1006-9321
543. Modeling of chemical vapor infiltration process for fabrication of carbon-carbon composites by finite difference methods , PERGAMON-ELSEVIER SCIENCE LTD,1999,37(4),669-677 ,DOI:10.1016/S0008-6223(98)00243-7, ISSN:0008-6223
544. Research on the distribution of the displacement in backward tube spinning , ELSEVIER SCIENCE SA,1998,79(1-3),185-188 ,DOI:10.1016/S0924-0136(98)00009-0, ISSN:0924-0136
545. 电子回旋共振推力器C/C复合材料栅极的力学性能 , Journal of Propulsion Technology, P.O. Box 7208-26, Beijing, 100074, China,2007,28(6),692-696 ,DOI:10.3321/j.issn:1001-4055.2007.06.022, ISSN:1001-4055
546. Cr含量对炭/炭复合材料SiC/Al-Si抗氧化涂层的影响 , 2010,39(z1),544-547 ,DOI:, ISSN:1002-185X
547. 退火对无序碳纳米管纯度及结构的影响 , 2007,36(z3),269-272 ,DOI:10.3321/j.issn:1002-185x.2007.z3.062, ISSN:1002-185X
548. 炭/炭复合材料硼硅酸盐玻璃涂层制备及性能研究 , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2010,(7),78-81,86 ,DOI:10.3969/j.issn.1001-4381.2010.07.017, ISSN:1001-4381
549. 碳纤维的分散性与CFRC复合材料的导电性 , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(10),1641-1644 ,DOI:10.3321/j.issn:1001-9731.2007.10.024, ISSN:1001-9731
550. 焦炭颗粒的粒度分布及其微观结构研究 , 2003,26(3),54-57 ,DOI:10.3969/j.issn.1004-4248.2003.03.011, ISSN:1004-4248
551. 硼酚醛树脂的制备和研究进展 , 2009,18(8),42-46 ,DOI:10.3969/j.issn.1004-2849.2009.08.011, ISSN:1004-2849
552. 用Ni-Ti粉末做中间层连接C/C复合材料和GH3128镍基高温合金 , NORTHWEST INST NONFERROUS METAL RESEARCH,2011,40(12),2088-2091 ,DOI:, ISSN:1002-185X
553. 炭/炭复合材料在1 680℃的抗氧化 , 2009,29(2),32-34 ,DOI:10.3969/j.issn.1007-1261.2009.02.010, ISSN:1007-1261
554. 炭/炭复合材料航空电刷的制备 , 2004,(3),3-6 ,DOI:10.3969/j.issn.1001-8948.2004.03.001, ISSN:1001-8948
555. 硅钽含量对C/C复合材料SiC/TaSi2复合涂层结构和抗氧化性能的影响 , 2009,38(z1),252-256 ,DOI:10.3321/j.issn:1002-185X.2009.z1.057, ISSN:1002-185X
556. 镍催化制备炭/炭复合材料 , 2004,23(3),17-21 ,DOI:10.3969/j.issn.1001-3741.2004.03.005, ISSN:1001-3741
557. 中间相沥青基炭/炭复合材料的微观结构与力学性能 , 2007,36(z3),331-334 ,DOI:10.3321/j.issn:1002-185x.2007.z3.077, ISSN:1002-185X
558. 声电沉积C/C磷灰石生物活性涂层的超声作用机制 , 2007,36(z3),594-598 ,DOI:10.3321/j.issn:1002-185x.2007.z3.143, ISSN:1002-185X
559. 催化剂对化学液相气化沉积制备炭/炭复合材料基体织构的影响 , 2007,36(z3),530-534 ,DOI:10.3321/j.issn:1002-185x.2007.z3.127, ISSN:1002-185X
560. 陶瓷复合材料的发展及其应用 , 2006,21(2),58-62 ,DOI:10.3969/j.issn.1009-5128.2006.02.017, ISSN:1009-5128
561. HfC改性炭/炭复合材料的烧蚀性能 , 2006,35(z1),365-368 ,DOI:10.3321/j.issn:1002-185X.2006.z1.089, ISSN:1002-185X
562. C/C复合材料等温CVI工艺模糊神经网络建模 , NORTHWEST INST NONFERROUS METAL RESEARCH,2004,33(10),1037-1040 ,DOI:10.3321/j.issn:1002-185X.2004.10.007, ISSN:1002-185X
563. 炭/炭复合材料高温力学行为研究 , SCIENCE CHINA PRESS,2003,18(1),20-24 ,DOI:10.3321/j.issn:1007-8827.2003.01.004, ISSN:1007-8827
564. 短切炭纤维增强沥青基C/C复合材料的组织特征 , SCIENCE CHINA PRESS,2004,19(2),119-123 ,DOI:10.3321/j.issn:1007-8827.2004.02.008, ISSN:1007-8827
565. 电流密度对声电沉积生物活性透钙磷石涂层结构和形貌的影响 , NORTHWEST INST NONFERROUS METAL RESEARCH,2003,32(11),923-926 ,DOI:10.3321/j.issn:1002-185X.2003.11.013, ISSN:1002-185X
566. CLVI制备C/C复合材料的微观结构及力学性能研究 , SCIENCE CHINA PRESS,2003,18(1),121-128 ,DOI:10.3321/j.issn:1000-324X.2003.01.019, ISSN:1000-324X
567. 低维GaN纳米材料的最新研究进展 , NORTHWEST INST NONFERROUS METAL RESEARCH,2002,31(5),321-324 ,DOI:10.3321/j.issn:1002-185X.2002.05.001, ISSN:1002-185X
568. Ni/Ti中间层部分瞬间液相法连接C/C复合材料和GH3044 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2012,35(3),414-418 ,DOI:10.3969/j.issn.1006-2793.2012.03.027, ISSN:1006-2793
569. C/C复合材料层间裂纹扩展研究 , SCIENCE CHINA PRESS,2002,17(1),91-95 ,DOI:10.3321/j.issn:1000-324X.2002.01.016, ISSN:1000-324X
570. 炭/炭复合材料高温防氧化陶瓷涂层的研究新进展 , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2010,(8),86-91 ,DOI:10.3969/j.issn.1001-4381.2010.08.019, ISSN:1001-4381
571. C/C复合材料难熔金属二硅化物涂层防氧化机理研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2010,33(2),218-221 ,DOI:10.3969/j.issn.1006-2793.2010.02.022, ISSN:1006-2793
572. 模压压力对焦炭颗粒增强沥青基炭复合材料性能的影响 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2009,32(5),559-564 ,DOI:10.3969/j.issn.1006-2793.2009.05.021, ISSN:1006-2793
573. 超短气体滞留时间制备C/C复合材料及其组织研究 , Beijing Institute of Aeronautical Materials (BIAM), P.O. Box 81, Beijing, 100095, China,2009,(9),33-37 ,DOI:10.3969/j.issn.1001-4381.2009.09.009, ISSN:1001-4381
574. 粗糙层组织结构2D-C/C复合材料的制备及特性 , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2009,23(2),138-142 ,DOI:10.3321/j.issn:1005-3093.2009.02.006, ISSN:1005-3093
575. C/C复合材料SiC/mullite-Si-Al2O3复合涂层微观结构及防氧化性能研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2009,32(2),226-229 ,DOI:10.3969/j.issn.1006-2793.2009.02.026, ISSN:1006-2793
576. 表面改性C/C复合材料与LAS玻璃陶瓷的连接 , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2009,30(2),380-384 ,DOI:10.3321/j.issn:1000-6893.2009.02.031, ISSN:1000-6893
577. 原位法制备C/C复合材料SiC/Si-Al2O3-mullite 复合抗氧化涂层 , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2009,30(3),551-556 ,DOI:10.3321/j.issn:1000-6893.2009.03.024, ISSN:1000-6893
578. 炭/炭复合材料SiC-MoSi2/SiC涂层结构及防氧化性能研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2008,31(6),638-641 ,DOI:10.3969/j.issn.1006-2793.2008.06.023, ISSN:1006-2793
579. 均化法对短炭纤维均匀化效果及C/C复合材料性能的影响 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2009,32(1),95-99 ,DOI:10.3969/j.issn.1006-2793.2009.01.022, ISSN:1006-2793
580. 硅钼含量对C/C复合材料SiC-MoSi2涂层结构和高温抗氧化性能的影响 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2008,31(3),283-287 ,DOI:10.3969/j.issn.1006-2793.2008.03.020, ISSN:1006-2793
581. 快速制备不同预制体C/C复合材料摩擦学性能研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2008,31(4),403-407 ,DOI:10.3969/j.issn.1006-2793.2008.04.023, ISSN:1006-2793
582. 化学液相汽化沉积法制备炭/炭复合材料的湿态摩擦磨损性能研究 , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2008,28(1),50-55 ,DOI:10.3321/j.issn:1004-0595.2008.01.010, ISSN:1004-0595
583. 炭/炭复合材料防氧化涂层研究进展 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2007,30(5),427-432 ,DOI:10.3969/j.issn.1006-2793.2007.05.016, ISSN:1006-2793
584. 石墨含量对纸基摩擦材料摩擦磨损性能的影响 , Science Press, 18,Shuangqing Street,Haidian, Beijing, 100085, China,2007,27(5),451-455 ,DOI:10.3321/j.issn:1004-0595.2007.05.011, ISSN:1004-0595
585. 化学液相气化沉积制备的炭/炭复合材料组织均匀性研究 , Journal of Solid Rocket Technology, P.O. Box 120, Xi'an, 710025, China,2007,30(5),437-441 ,DOI:10.3969/j.issn.1006-2793.2007.05.018, ISSN:1006-2793
586. 等离子喷涂炭/炭复合材料Cr-Al-Si涂层显微结构及高温抗氧化性能 , Beijing University of Aeronautics and Astronautics (BUAA), 37 Xueyuan Rd., Haidian District, Beijing, 100083, China,2007,24(5),109-112 ,DOI:10.3321/j.issn:1000-3851.2007.05.020, ISSN:1000-3851
587. 包埋法制备碳/碳复合材料碳化硅涂层缺陷的形成机制及控制 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2007,35(6),721-724 ,DOI:10.3321/j.issn:0454-5648.2007.06.011, ISSN:0454-5648
588. 碳纤维诱导法制备SiC晶须的工艺及机理 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2007,35(5),643-647 ,DOI:10.3321/j.issn:0454-5648.2007.05.023, ISSN:0454-5648
589. 声电沉积-氟化钠处理复合工艺制备C/C含氟磷灰石涂层 , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(8),1320-1323,1326 ,DOI:10.3321/j.issn:1001-9731.2007.08.030, ISSN:1001-9731
590. 涂层碳/碳复合材料氧化机理的研究 , Journal of Functional Materials, P.O. Box 1512, Chongqing, 630700, China,2007,38(8),1327-1330 ,DOI:10.3321/j.issn:1001-9731.2007.08.032, ISSN:1001-9731
591. 用碳化稻壳制备碳/碳复合材料的SiC涂层 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, 100095, China,2007,(6),11-14 ,DOI:10.3969/j.issn.1001-4381.2007.06.003, ISSN:1001-4381
592. 碳/碳复合材料SiC/Al-Si涂层微观结构及抗氧化性能研究 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2007,(4),43-46 ,DOI:10.3969/j.issn.1001-4381.2007.04.011, ISSN:1001-4381
593. 三维编织复合材料预制体孔隙的几何仿真 , Chinese Journal of Materials Research, 72 Wenhua Road, Shenyang, 110015, China,2007,21(2),161-165 ,DOI:10.3321/j.issn:1005-3093.2007.02.010, ISSN:1005-3093
594. 三维编织复合材料矩形预制件仿真 , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2006,27(5),985-988 ,DOI:10.3321/j.issn:1000-6893.2006.05.049, ISSN:1000-6893
595. 炭化压力对沥青成焦组织和形貌的影响 , AAAS Press of Chinese Society of Aeronautics and, P.O. Box 399, Beijing, China,2006,27(5),969-972 ,DOI:10.3321/j.issn:1000-6893.2006.05.046, ISSN:1000-6893
596. 碳/碳复合材料表面聚四氟乙烯复合涂层的摩擦学性能 , 2006,40(1),72-74,105 ,DOI:10.3321/j.issn:0253-987X.2006.01.017, ISSN:0253-987X
597. 纤维含量和热处理对炭/炭复合材料性能的影响 , Chinese Journal of Materials Research,2005,19(3),293-298 ,DOI:10.3321/j.issn:1005-3093.2005.03.012, ISSN:1005-3093
598. 多孔阳极氧化铝薄膜的制备 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2005,0(5),56-59,64 ,DOI:10.3969/j.issn.1001-4381.2005.05.015, ISSN:1001-4381
599. 热处理温度对钼酚醛树脂连接炭/炭复合材料接头性能的影响 , Editorial Office of Transactions of Materials and Heat Treatment,2005,26(4),5-7 ,DOI:10.3969/j.issn.1009-6264.2005.04.003, ISSN:1009-6264
600. 碳/碳复合材料摩擦学性能及摩擦机制研究进展 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2004,0(12),59-62 ,DOI:10.3969/j.issn.1001-4381.2004.12.015, ISSN:1001-4381
601. 沉积位置对化学气相沉积SiC涂层微观组织的影响 , 2005,39(1),49-52 ,DOI:10.3321/j.issn:0253-987X.2005.01.012, ISSN:0253-987X
602. 三维编织复合材料的力学性能研究现状 , Beijing Institute of Aeronautical Materials (BIAM),2004,0(2),44-48 ,DOI:10.3969/j.issn.1001-4381.2004.02.012, ISSN:1001-4381
603. C/C复合材料等温CVI工艺Mamdani模糊系统建模 , Chinese Journal of Materials Research,2003,17(4),375-379 ,DOI:10.3321/j.issn:1005-3093.2003.04.007, ISSN:1005-3093
604. 碳/碳复合材料等温化学气相渗透工艺模糊系统建模 , Chinese Ceramic Society,2003,31(7),629-634 ,DOI:10.3321/j.issn:0454-5648.2003.07.002, ISSN:0454-5648
605. 生物医用碳/碳复合材料碳化硅涂层的研究 , 2003,21(3),356-359 ,DOI:10.3969/j.issn.1000-2758.2003.03.027, ISSN:1000-2758
606. 碳/碳复合材料等温CVI工艺有限元模拟及可视化研究 , 2003,21(3),360-363 ,DOI:10.3969/j.issn.1000-2758.2003.03.028, ISSN:1000-2758
607. SiC改性C/C复合材料的制备及其烧蚀性能 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2011,39(2),251-255 ,DOI:, ISSN:0454-5648
608. 高温对碳/碳复合材料性能影响的研究 , 2003,21(3),352-355 ,DOI:10.3969/j.issn.1000-2758.2003.03.026, ISSN:1000-2758
609. 基体改性对碳/碳复合材料烧蚀率影响的神经网络模拟 , 2003,37(3),249-251,330 ,DOI:10.3321/j.issn:0253-987X.2003.03.008, ISSN:0253-987X
610. 快速液相气化法制备碳/碳复合材料研究进展 , 2002,30(4),513-516 ,DOI:10.3321/j.issn:0454-5648.2002.04.022, ISSN:0454-5648
611. 碳/碳生物活性玻璃涂层复合材料的组织结构研究 , 2002,20(4),612-615 ,DOI:10.3969/j.issn.1000-2758.2002.04.023, ISSN:1000-2758
612. 国内外C/C复合材料疲劳性能的研究进展 , 2011,25(7),63-66 ,DOI:, ISSN:1005-023X
613. 料浆法制备碳/碳复合材料Al-Si合金抗氧化涂层 , 2010,39(18),87-89 ,DOI:10.3969/j.issn.1001-3814.2010.18.024, ISSN:1001-3814
614. 碳/碳复合材料SiC/W-Al-Si涂层微观结构及抗氧化性能 , Editorial Office of Transactions of Materials, 18 Xueqing Road, Beijing, 100083, China,2011,32(7),17-20 ,DOI:, ISSN:1009-6264
615. SiC-CVD过程的人工神经网络建模 , Chinese Ceramic Society, China,2000,28(1),25-29 ,DOI:10.3321/j.issn:0454-5648.2000.01.006, ISSN:0454-5648
616. 碳纤维增强碳复合材料高温抗氧化硅基陶瓷涂层的研究进展 , Chinese Ceramic Society, Baiwanzhuang, Beijing, 100831, China,2010,38(5),991-996 ,DOI:, ISSN:0454-5648
617. 两步包埋法制备C/C复合材料SiC/Cr-Al-Si涂层研究 , 2009,24(2),89-92 ,DOI:10.3969/j.issn.1673-064X.2009.02.024, ISSN:1673-064X
618. 国内外碳/碳复合材料连接研究进展 , 2009,23(7),9-12 ,DOI:10.3321/j.issn:1005-023X.2009.07.003, ISSN:1005-023X
619. 单向碳/碳复合材料CVI致密化模拟研究 , 1999,16(2),129-134 ,DOI:10.3321/j.issn:1000-3851.1999.02.025, ISSN:1000-3851
620. C/C复合材料SiC/W-Mo-Si抗氧化复合涂层研究 , 2008,41(2),43-46 ,DOI:, ISSN:1001-1560
621. 电沉积制备羟基磷灰石-碳化硅复合涂层 , 2008,30(9),4-8 ,DOI:10.3969/j.issn.1001-3849.2008.09.002, ISSN:1001-3849
622. 人工髋关节假体材料的研究进展 , 2008,22(4),108-111 ,DOI:10.3321/j.issn:1005-023X.2008.04.027, ISSN:1005-023X
623. 碳纤维增强水泥基复合材料的电磁屏蔽性能 , 2008,25(6),536-540,544 ,DOI:10.3321/j.issn:1003-5214.2008.06.005, ISSN:1003-5214
624. CVI处理短碳纤维在CFRC中分散性的评价 , 2008,26(1),20-26 ,DOI:, ISSN:1673-2812
625. 基于有限元的C/C燃气舵振动特性 , 2011,(1),12-15 ,DOI:10.3969/j.issn.1003-0999.2011.01.003, ISSN:1003-0999
626. 短碳纤维在不同分散剂中的分散性 , 2007,24(1),1-4,26 ,DOI:10.3321/j.issn:1003-5214.2007.01.001, ISSN:1003-5214
627. 双基体炭/炭复合材料的微观结构与力学性能 , 2008,26(1),8-11 ,DOI:, ISSN:1673-2812
628. 短碳纤维的分散性与CFRC复合材料的力学性能 , 2007,24(6),521-525 ,DOI:10.3321/j.issn:1003-5214.2007.06.001, ISSN:1003-5214
629. Ni71 CrSi 中间层钎焊连接 C/C 复合材料与镍基高温合金 GH3044 , 2013,32(11),665-670 ,DOI:10.7502/j.issn.1674-3962.2013.11.05, ISSN:1674-3962
630. 航天器热防护材料研究现状与发展趋势 , 2007,21(8),15-18 ,DOI:10.3321/j.issn:1005-023X.2007.08.004, ISSN:1005-023X
631. 用气相反应法制备C/C复合材料的梯度SiC涂层 , 2007,25(2),175-178 ,DOI:10.3969/j.issn.1673-2812.2007.02.003, ISSN:1673-2812
632. 催化裂解无水乙醇制备纳米碳管 , 2007,26(4),445-448 ,DOI:10.3321/j.issn:1003-8728.2007.04.012, ISSN:1003-8728
633. 炭纤维增强水泥基复合材料(CFRC)的电磁性能 , 2010,29(1),33-40 ,DOI:10.3969/j.issn.1001-3741.2010.01.008, ISSN:1001-3741
634. 碳密封材料的研究进展及其在航空航天领域的应用 , 2006,36(4),12-17 ,DOI:10.3969/j.issn.1007-2330.2006.04.003, ISSN:1007-2330
635. 应力水平对3D C/C复合材料的弯弯疲劳损伤模式的影响 , 2007,37(1),53-59 ,DOI:10.3321/j.issn:1006-9275.2007.01.008, ISSN:1006-9275
636. C/C复合材料与金属材料的热压连接 , 2009,28(5),27-30 ,DOI:10.3969/j.issn.1001-3741.2009.05.006, ISSN:1001-3741
637. 催化裂解简单合成离散的短纳米碳管 , 2006,19(5),2348-2350 ,DOI:10.3969/j.issn.1004-1699.2006.05.275, ISSN:1004-1699
638. 电气石/无机抗菌剂复合型中空活性碳纤维研究 , 2006,29(4),22-24,45 ,DOI:10.3969/j.issn.1000-8098.2006.04.007, ISSN:1000-8098
639. C/C复合材料CVI工艺的计算机模拟研究进展 , 2006,36(4),7-11 ,DOI:10.3969/j.issn.1007-2330.2006.04.002, ISSN:1007-2330
640. 不同转速及载荷下炭/炭复合材料的摩擦磨损性能 , 2006,24(3),330-333,357 ,DOI:10.3969/j.issn.1673-2812.2006.03.002, ISSN:1673-2812
641. C/C复合材料比热容和热扩散率的研究 , 2005,35(6),41-43 ,DOI:10.3969/j.issn.1007-2330.2005.06.009, ISSN:1007-2330
642. TG-CVI C/C复合材料裂纹缺陷成因分析 , 2009,28(1),26-29 ,DOI:10.3969/j.issn.1001-3741.2009.01.007, ISSN:1001-3741
643. 国内C/C复合材料基体改性研究进展 , 2011,30(11),6-12,39 ,DOI:, ISSN:1674-3962
644. 控制润滑状态下纸基摩擦材料的摩擦特性研究 , Science Press,2005,(3),40-43 ,DOI:10.3969/j.issn.0254-0150.2005.03.014, ISSN:0254-0150
645. 碳/碳复合材料的疲劳行为研究 , 2005,23(3),453-456 ,DOI:10.3969/j.issn.1673-2812.2005.03.036, ISSN:1673-2812
646. 模压工艺制备短纤维增强C/C复合材料的研究 , 2004,34(6),11-15 ,DOI:10.3969/j.issn.1007-2330.2004.06.003, ISSN:1007-2330
647. 毡基和碳布叠层C/C复合材料的高温力学及抗氧化性能比较 , 2005,24(7),781-784 ,DOI:10.3321/j.issn:1003-8728.2005.07.007, ISSN:1003-8728
648. 炭/炭复合材料CVI工艺的数值模拟现状 , 2005,19(5),58-60,69 ,DOI:10.3321/j.issn:1005-023X.2005.05.017, ISSN:1005-023X
649. 一种新型短切碳纤维增强纸基摩擦材料研究 , 2004,22(6),802-805 ,DOI:10.3969/j.issn.1673-2812.2004.06.006, ISSN:1673-2812
650. ICVI制备炭/炭复合材料流场模拟 , 2008,8(11),2786-2792 ,DOI:10.3969/j.issn.1671-1815.2008.11.007, ISSN:1671-1815
651. 预制体添加BN对炭/炭复合材料性能的影响 , 2010,29(1),36-39 ,DOI:, ISSN:1003-8728
652. 三维编织碳/碳复合材料预制体结构模拟 , 2004,22(5),634-636 ,DOI:10.3969/j.issn.1673-2812.2004.05.003, ISSN:1673-2812
653. 碳纳米管合成进展 , 2004,18(9),43-46 ,DOI:10.3321/j.issn:1005-023X.2004.09.014, ISSN:1005-023X
654. 热解炭结构对C/C复合材料热物理性能影响 , 2007,26(5),10-13 ,DOI:10.3969/j.issn.1001-3741.2007.05.003, ISSN:1001-3741
655. 炭/炭复合材料表面高温抗氧化合金涂层的研究进展 , 2011,44(2),36-39,69 ,DOI:, ISSN:1001-1560
656. 焦炭颗粒/热解炭复合材料的制备与压缩性能研究 , 2013,32(3),12-16 ,DOI:, ISSN:1001-3741
657. C/C复合材料等温CVI工艺T-S模糊系统研究 , China Spaceflight Society, Beijing, China,2004,25(1),119-122 ,DOI:10.3321/j.issn:1000-1328.2004.01.021, ISSN:1000-1328
658. 软计算在材料性能预测建模中的应用 , 2004,23(1),77-80 ,DOI:10.3321/j.issn:1003-8728.2004.01.025, ISSN:1003-8728
659. C/C复合材料CVI工艺人工神经网络建模 , 2003,33(3),209-216 ,DOI:10.3321/j.issn:1006-9275.2003.03.004, ISSN:1006-9275
660. 沥青基炭复合材料的制备及力学各向异性性质的探讨 , 2006,25(5),1-4 ,DOI:10.3969/j.issn.1001-3741.2006.05.001, ISSN:1001-3741
661. 软计算技术在热处理中的应用 , 2003,28(6),42-45 ,DOI:10.3969/j.issn.0254-6051.2003.06.014, ISSN:0254-6051
662. 软计算在CVD/CVI工艺建模中的应用 , 2003,17(5),12-14 ,DOI:10.3321/j.issn:1005-023X.2003.05.004, ISSN:1005-023X
663. 电镀用锌镍合金阳极的研制及应用 , 2002,51(9),554-556 ,DOI:10.3321/j.issn:1001-4977.2002.09.011, ISSN:1001-4977
664. 沥青种类和焦炭粒度组成对焦炭颗粒增强沥青基炭复合材料性能的影响 , 2005,24(5),15-19 ,DOI:10.3969/j.issn.1001-3741.2005.05.004, ISSN:1001-3741
665. 酞菁组分和硫粉量对直立碳纳米管生长的影响 , 2009,28(10),1344-1348 ,DOI:, ISSN:1003-8728
666. 三维编织碳/碳复合材料(C/C)的拉伸性能及损伤 , 2002,21(3),451-453 ,DOI:10.3321/j.issn:1003-8728.2002.03.039, ISSN:1003-8728
667. 钨酚醛树脂连接炭/炭复合材料的工艺研究 , 2005,24(2),17-20 ,DOI:10.3969/j.issn.1001-3741.2005.02.005, ISSN:1001-3741
668. 热梯度化学气相沉积工艺制备炭/炭复合材料 , 2005,(6),71-73 ,DOI:10.3969/j.issn.1003-5311.2005.06.029, ISSN:1003-5311
669. 液相气化法制备碳/碳复合材料工艺研究 , 2002,21(1),99-101 ,DOI:10.3321/j.issn:1003-8728.2002.01.036, ISSN:1003-8728
670. 人工神经网络在复合材料研究中的应用 , 2003,23(4),13-18 ,DOI:10.3969/j.issn.1000-7202.2003.04.003, ISSN:1000-7202
671. 短碳纤维复合材料中纤维均匀化技术的研究现状 , 2003,26(6),50-53 ,DOI:10.3969/j.issn.1004-244X.2003.06.013, ISSN:1004-244X
672. 炭/炭复合材料研究应用现状及思考 , 2001,0(5),24-27 ,DOI:10.3969/j.issn.1001-3741.2001.05.007, ISSN:1001-3741
673. 2D碳/碳复合材料CVI过程的数值模拟研究 , China Spaceflight Soc, China,1999,20(4),104-107 ,DOI:10.3321/j.issn:1000-1328.1999.04.018, ISSN:1000-1328
674. 高温下炭/炭复合材料对钛合金组织及性能的影响 , 2003,0(3),6-9 ,DOI:10.3969/j.issn.1001-3741.2003.03.002, ISSN:1001-3741
675. 我国炭/炭复合材料研究进展 , 2001,(4),8-13 ,DOI:10.3969/j.issn.1001-8948.2001.04.004, ISSN:1001-8948
676. Effect of heat treatment temperature on the fracture characteristics of carbon/carbon composite discs , TRANS TECH PUBLICATIONS LTD,2006,324-325,519-522 ,DOI:, ISSN:1013-9826
677. C/C复合材料航空电刷的制备 , 2004,(中国海口),47-50 ,DOI:, ISSN:
678. 炭/炭复合材料Ir-Al-Si涂层微观结构及抗氧化性能研究 , 2007,,350-353 ,DOI:, ISSN:
679. 碳/碳复合材料高温抗氧化涂层研究新进展 , 2006,(中国四川成都),15-21 ,DOI:, ISSN:
680. 六棱柱状SiC纳米线的制备与表征 , 2005,(中国山东省烟台市),577-582 ,DOI:, ISSN:
681. 炭/炭复合材料磷酸盐涂层的抗氧化性能研究 , 2004,(中国海口),95-100 ,DOI:, ISSN:
682. 专家系统在复合材料研究中的应用 , 2002,(中国天津),1025-1029 ,DOI:, ISSN:
683. 声电沉积制备碳/碳复合材料生物活性透钙磷石涂层研究 , 2002,(中国天津),60-64 ,DOI:, ISSN:
684. 筒形件反旋时工艺参数对残余应力分布的影响 , 1997,22(04),23-25+36 ,DOI:, ISSN:1000-3940
685. 筒形件正旋时工艺参数对残余应力分布的影响 , 1997,(04),44-47 ,DOI:, ISSN:1004-244X
686. 筒形件强力旋压变形中的应力应变分布 , 1997,5(1),12 ,DOI:, ISSN:1005-0930
687. 筒形件强力旋压时金属切向变形分析 , NPU, Xi'an, China,1998,16(4),627 ,DOI:, ISSN:1000-2758
688. 旋压筒形件残余应力的数值模拟 , 1998,(03),60-63 ,DOI:, ISSN:1007-2012
689. CVI制备碳/碳复合材料致密化行为模拟研究 , 1999,22(2),28 ,DOI:, ISSN:1004-244X
690. C/C复合材料热梯度CVI工艺的数值模拟研究 , Beijing University of Aeronautics and Astronautics (BUAA),2000,17(4),84 ,DOI:, ISSN:1000-3851
691. 轴对称C/C复合材料件等温CVI过程的数值模拟研究 , 2000,18(4),665 ,DOI:, ISSN:1000-2758
692. C/C复合材料正压CVI工艺的实验探索 , 2000,0(6),13 ,DOI:, ISSN:1001-3741
693. 我国碳/碳复合材料研究进展 , 2000,,1 ,DOI:, ISSN:
694. 液相气化快速致密化工艺研究 , 2001,0(6),1 ,DOI:, ISSN:1001-3741
695. 炭/炭复合材料磷酸盐涂层的抗氧化性能研究 , 2005,38(3),52-54 ,DOI:, ISSN:1001-1560
696. 化学气相沉积制备MoSi2涂层分析 , 2005,19(7),37-40 ,DOI:, ISSN:1005-023X
697. 应力水平对3DC/C复合材料的弯弯疲劳损伤模式的影响 , 2007,37(1),53-59 ,DOI:, ISSN:1006-9275
698. 中间相沥青基炭/炭复合材料的微观结构与力学性能(英文) , 2007,(S3),331-334 ,DOI:, ISSN:1002-185X
699. 高压浸渍-炭化制备炭/炭复合材料的组织结构 , Harbin Institute of Technology, P.O. Box 136, Harbin, 150001, China,2008,16(6),755-758 ,DOI:, ISSN:1005-0299
700. 包埋工艺参数对碳/碳复合材料表面SiC涂层致密性的影响 , 2009,33(3),5 ,DOI:, ISSN:1000-3738
701. TCVI工艺制备C/C复合材料的多物理场耦合模拟 , 2009,39(11),1804-1809 ,DOI:, ISSN:1006-9275
702. Cr含量对炭/炭复合材料SiC/Al-Si抗氧化涂层的影响(英文) , 2010,(S1),544-547 ,DOI:, ISSN:1002-185X
703. HfC-SiC改性炭/炭复合材料的制备方法 , 2014, ,DOI:, ISSN:
704. 不同温度热处理对CVI-C/C复合材料力学性能的影响 , 2010,(中国湖南长沙),6 ,DOI:, ISSN:
705. 炭/炭复合材料C/SiC/MoSi_2-SiC-Si抗氧化复合涂层(英文) , ELSEVIER SCIENCE BV,2013,23(07),2118-2122 ,DOI:10.1016/S1003-6326(13)62705-3, ISSN:1003-6326
706. 氧化镁-钇铝石榴石纤维晶粒生长动力学研究 , 2014,(中国广东清远),1 ,DOI:, ISSN:
707. 一种介电电泳技术制备碳纳米管/碳/碳复合材料的方法 , 2013, ,DOI:, ISSN:
708. 一种硼锆硅三元改性酚醛树脂及其制备方法 , 2013, ,DOI:, ISSN:
709. 一种C/C复合材料和镍基高温合金的高温钎焊连接方法 , 2013, ,DOI:, ISSN:
710. 一种镍/氧化镍修饰氮掺杂石墨烯材料的制备方法 , 2013, ,DOI:, ISSN:
711. 一种各向同性热解碳的制备方法 , 2013, ,DOI:, ISSN:
712. 碳/碳-碳化锆复合材料的制备方法 , 2013, ,DOI:, ISSN:
713. 碳纤维-氧化石墨烯-碳纳米管多尺度增强体的制备方法 , 2013, ,DOI:, ISSN:
714. 一种珠串状纳米线增韧增强陶瓷涂层的制备方法 , 2013, ,DOI:, ISSN:
715. 一种炭/炭复合材料的制备方法 , 2013, ,DOI:, ISSN:
716. 一种锆改性酚醛树脂及其制备方法 , 2013, ,DOI:, ISSN:
717. 提高炭/炭复合材料—锂铝硅陶瓷接头连接性能的方法 , 2013, ,DOI:, ISSN:
718. 碳/碳复合材料与镍基高温合金的部分瞬间液相连接方法 , 2013, ,DOI:, ISSN:
719. 碳纤维表面生物活化改性方法 , 2013, ,DOI:, ISSN:
720. 一种提高碳/碳复合材料与自身连接性能的方法 , 2013, ,DOI:, ISSN:
721. 一种超长纳米线增韧陶瓷涂层的制备方法 , 2013, ,DOI:, ISSN:
722. 碳泡沫/羟基磷灰石复合涂层的制备方法 , 2012, ,DOI:, ISSN:
723. 炭/炭复合材料的表面氧化改性方法 , 2012, ,DOI:, ISSN:
724. 纳米线增强羟基磷灰石涂层的制备方法 , 2012, ,DOI:, ISSN:
725. 纳米碳基燃料电池催化剂的制备方法 , 2012, ,DOI:, ISSN:
726. 化学气相沉积法制备同轴碳化硅/二氧化硅纳米电缆的方法 , 2012, ,DOI:, ISSN:
727. 炭/炭-铜复合材料的制备方法 , 2012, ,DOI:, ISSN:
728. 一种炭/炭复合材料宽温域防氧化硅基陶瓷涂层的制备方法 , 2012, ,DOI:, ISSN:
729. 一种制备Al掺杂的碳化硅纳米线的方法 , 2012, ,DOI:, ISSN:
730. 一种纳米带增韧硅基陶瓷涂层的制备方法 , 2012, ,DOI:, ISSN:
731. 四氧化三铁/碳纳米管复合材料的制备方法 , 2012, ,DOI:, ISSN:
732. 碳纤维/氧化锆纳米线混杂增强材料的其制备方法 , 2012, ,DOI:, ISSN:
733. 一种硼化铪HfB2抗烧蚀粉体的制备方法 , 2012, ,DOI:, ISSN:
734. 一种在SiC陶瓷表面制备碳化硅纳米带的方法 , 2011, ,DOI:, ISSN:
735. 一种制备SiC纳米线和纳米带的方法 , 2011, ,DOI:, ISSN:
736. 炭/炭复合材料SiC/ZrB2-SiC/SiC涂层及其制备方法 , 2011, ,DOI:, ISSN:
737. 稀土增韧炭/炭复合材料的制备方法 , 2011, ,DOI:, ISSN:
738. 碳/碳复合材料表面的氧化处理方法 , 2011, ,DOI:, ISSN:
739. 一种制备竹节状SiC纳米线增韧HfC陶瓷的方法 , 2011, ,DOI:, ISSN:
740. 一种制备中间相沥青基炭/炭复合材料的方法 , 2010, ,DOI:, ISSN:
741. 重载差速器用湿式摩擦材料及其制备方法 , 2010, ,DOI:, ISSN:
742. 橡胶-树脂共混型纸基摩擦材料 , 2010, ,DOI:, ISSN:
743. 碳纤维增强碳-碳化硅双基体材料的制备方法 , 2010, ,DOI:, ISSN:
744. 一种纳米线增韧碳/碳复合材料陶瓷涂层的制备方法 , 2010, ,DOI:, ISSN:
745. 在碳/碳复合材料表面制备碳化硅-焦硅酸镱复合涂层的方法 , 2010, ,DOI:, ISSN:
746. C/C复合材料表面防氧化SiC/mullite-Si-Al2O3复合涂层的制备方法 , 2009, ,DOI:, ISSN:
747. 碳/碳复合材料防氧化涂层的制备方法 , 2009, ,DOI:, ISSN:
748. 碳/碳复合材料与镍基高温合金的连接方法 , 2009, ,DOI:, ISSN:
749. 大尺寸各向同性热解炭的制备方法 , 2008, ,DOI:, ISSN:
750. 碳/碳复合材料表面高温防氧化涂层的制备方法 , 2008, ,DOI:, ISSN:
751. 炭/炭复合材料ZrC抗烧蚀涂层的制备方法 , 2008, ,DOI:, ISSN:
752. 碳化硅纳米线的制备方法 , 2008, ,DOI:, ISSN:
753. 柔性纸基摩擦材料 , 2007, ,DOI:, ISSN:
754. 碳纤维与热解碳基体中间相沥青过渡层复合材料的制备方法 , 2006, ,DOI:, ISSN:
755. 碳纳米管纯化方法 , 2006, ,DOI:, ISSN:
756. 在碳布基底上生长碳纳米管的方法 , 2006, ,DOI:, ISSN:
757. 有序碳纳米管阵列的制备方法 , 2006, ,DOI:, ISSN:
758. 碳/碳复合材料表面抗氧化多相涂层的制备方法 , 2006, ,DOI:, ISSN:
759. 碳/碳复合材料的连接方法 , 2006, ,DOI:, ISSN:
760. 在碳/碳复合材料表面制备碳化硅涂层的方法 , 2005, ,DOI:, ISSN:
761. 大功率热梯度化学气相渗透工艺系统监控装置及监控方法 , 2005, ,DOI:, ISSN:
762. 碳化硅晶须生成炉及生产碳化硅晶须的方法 , 2005, ,DOI:, ISSN:
763. 三氧化二硼-碳化硅自润滑涂层及其制备方法 , 2005, ,DOI:, ISSN:
764. 碳/碳复合材料表面碳化硅纳米线的制备方法 , 2005, ,DOI:, ISSN:
765. 碳/碳复合材料热梯度化学气相渗透过程温度自动控制器 , 2005, ,DOI:, ISSN:
766. 接头剪切强度测试夹具 , 2004, ,DOI:, ISSN:
767. 热梯度化学气相沉积法制备炭/炭复合材料 , 2004, ,DOI:, ISSN:
768. 自热法制备炭/炭复合材料实心圆柱体制件 , 2004, ,DOI:, ISSN:
769. 热梯度化学气相沉积法制备炭/炭复合材料厚壁板材 , 2004, ,DOI:, ISSN:
770. 炭/炭复合材料异型螺旋管 , 2004, ,DOI:, ISSN:
771. 模压半炭化成型方法制备炭素材料 , 2004, ,DOI:, ISSN:
772. 碳纤维增强纸基摩擦材料及其制备方法 , 2003, ,DOI:, ISSN:
773. 石墨层间化合物增韧热解碳基复合材料方法 , 2001, ,DOI:, ISSN:
774. 限域变温压差化学气相渗透工艺 , 2000, ,DOI:, ISSN:
775. Preparation and oxidation kinetics mechanism of three-layer multi-layer-coatings-coated carbon/carbon composites , Elsevier,2006,200(18-19),5379-5385 ,DOI:10.1016/j.surfcoat.2005.06.011, ISSN:02578972
776. Directional thermophysical, ablative and compressive behavior of 3D carbon/carbon composites , ELSEVIER SCI LTD,2015,41(8),9763-9769 ,DOI:10.1016/j.ceramint.2015.04.048, ISSN:0272-8842
777. Prefabrication of SiC whiskers through induction of carbon fiber , ALLERTON PRESS INC,2006,16(,1),S483-S486 ,DOI:10.1016/S1003-6326(06)60239-2, ISSN:1003-6326
778. Ablation behaviour of C/C-ZrC composites in a solid rocket motor environment , ELSEVIER SCI LTD,2015,41(9),11793-11803 ,DOI:10.1016/j.ceramint.2015.05.147, ISSN:0272-8842
779. ZrO_2添加量对Al_2O_3/ZrO_2复相陶瓷性能的影响 , 2015,38(4),37-40 ,DOI:, ISSN:1004-244X
780. C/C-ZrC复合材料的微观结构和力学性能研究 , SCIENCE PRESS,2015,30(05),459-466 ,DOI:10.15541/jim20140455, ISSN:1000-324X
781. 复合工艺制备炭/炭密封材料弯曲断裂特征 , 2006,35(z1),245-248 ,DOI:10.3321/j.issn:1002-185X.2006.z1.061, ISSN:1002-185X
782. 预炭层对ZrC浸渍C/C复合材料微观结构和力学性能的影响 , ELSEVIER SCIENCE BV,2015,30(04),372-377 ,DOI:, ISSN:1007-8827
783. C/C复合材料SiC涂层强冲蚀环境的烧蚀性能研究 , 2015,34(7),610-614 ,DOI:10.7502/j.issn.1674-3962.2015.07.17, ISSN:1674-3962
784. In vitro mineralization of MC3T3-E1 osteoblast-like cells on collagen/nano-hydroxyapatite scaffolds coated carbon/carbon composites , WILEY-BLACKWELL,2016,104(2),533-543 ,DOI:10.1002/jbm.a.35593, ISSN:1549-3296
785. Oxidation protective glass coating for SiC coated carbon/carbon composites for application at 1773 K , ELSEVIER SCIENCE BV,2006,60(3),431-434 ,DOI:10.1016/j.matlet.2005.09.006, ISSN:0167-577X
786. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2006,44(3),602-605 ,DOI:10.1016/j.carbon.2005.09.026, ISSN:0008-6223
787. Growth and morphology of one-dimensional SiC nanostructures without catalyst assistant , ELSEVIER SCIENCE SA,2006,95(1),140-144 ,DOI:10.1016/j.matchemphys.2005.05.032, ISSN:0254-0584
788. Microstructure and growth mechanism of SiC whiskers on carbon/carbon composites prepared by CVD , ELSEVIER SCIENCE BV,2005,59(19-20),2593-2597 ,DOI:10.1016/j.matlet.2005.02.088, ISSN:0167-577X
789. Double-layer oxidation protective SIC/glass coatings for carbon/carbon composites , ELSEVIER SCIENCE SA,2006,200(11),3473-3477 ,DOI:10.1016/j.surfcoat.2004.11.022, ISSN:0257-8972
790. The influence of thermal gradient on pyrocarbon deposition in carbon/carbon composites during the CVI process , PERGAMON-ELSEVIER SCIENCE LTD,2006,44(4),786-791 ,DOI:10.1016/j.carbon.2005.08.030, ISSN:0008-6223
791. The thermal expansion of carbon/carbon composites from room temperature to 1400 degrees C , SPRINGER,2006,41(24),8356-8358 ,DOI:10.1007/s10853-006-1073-9, ISSN:0022-2461
792. SiC-MoSi2-(Ti0.8Mo0.2)Si-2 multi-composition coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2006,201(6),3452-3456 ,DOI:10.1016/j.surfcoat.2006.07.237, ISSN:0257-8972
793. Synthesis of silicon carbide nanowires by CVD without using a metallic catalyst , ELSEVIER SCIENCE SA,2006,100(1),108-111 ,DOI:10.1016/j.matchemphys.2005.12.014, ISSN:0254-0584
794. Prefabrication of SiC whiskers through induction of carbon fiber , Nonferrous Metals Society of China, B12 Fuxing Road, Beijing, 100814, China,2006,16(SUPPL. 1),483-486 ,DOI:10.1016/S1003-6326(06)60083-6, ISSN:10036326
795. 炭/炭复合材料新型热梯度制备工艺 , SCIENCE CHINA PRESS,2007,22(3),247-252 ,DOI:10.3969/j.issn.1007-8827.2007.03.009, ISSN:1007-8827
796. Microstructures and mechanical properties of carbon/carbon composites reinforced with carbon nanofibers/nanotubes produced in situ , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(8),1662-1668 ,DOI:10.1016/j.carbon.2007.03.042, ISSN:0008-6223
797. Double-layer oxidation protective SiC/Cr-Al-Si coating for carbon-carbon composites , ELSEVIER SCIENCE SA,2007,201(18),7842-7846 ,DOI:10.1016/j.surfcoat.2007.03.025, ISSN:0257-8972
798. Photoluminescence of hexagonal-shaped SiC nanowires prepared by sol-gel process , ELSEVIER SCIENCE SA,2007,460,233-237 ,DOI:10.1016/j.msea.2007.02.025, ISSN:0921-5093
799. The influence of SiC coating process on the properties of C/C composites , WORLD SCIENTIFIC PUBL CO PTE LTD,2007,14(4),817-820 ,DOI:10.1142/S0218625X07010317, ISSN:0218-625X
800. MoSi2-improved SiC coating to protect carbon/carbon composites against oxidation , WORLD SCIENTIFIC PUBL CO PTE LTD,2007,14(4),795-799 ,DOI:10.1142/S0218625X07010093, ISSN:0218-625X
801. In situ catalytic growth of carbon nanotubes on the surface of carbon cloth , ELSEVIER SCI LTD,2007,67(14),2986-2989 ,DOI:10.1016/j.compscitech.2007.05.002, ISSN:0266-3538
802. Effect of chemical vapor deposition treatment of carbon fibers on the reflectivity of carbon fiber-reinforced cement-based composites , ELSEVIER SCI LTD,2008,68(5),1105-1114 ,DOI:10.1016/j.compscitech.2007.08.003, ISSN:0266-3538
803. Application of microcapsulation technology to the preparation of carbon foam , NATL INST MATERIALS SCIENCE,2008,9(2) ,DOI:10.1088/1468-6996/9/2/025011, ISSN:1468-6996
804. Effect of carbon fiber dispersion on the mechanical properties of carbon fiber-reinforced cement-based composites , ELSEVIER SCIENCE SA,2008,487(1-2),52-57 ,DOI:10.1016/j.msea.2007.09.073, ISSN:0921-5093
805. Influence of CVI treatment of carbon fibers on the electromagnetic interference of CFRC composites , ELSEVIER SCI LTD,2008,30(6),478-485 ,DOI:10.1016/j.cemconcomp.2007.09.002, ISSN:0958-9465
806. High Performance SiC Oxidation Protective Coating with ZrO2 Particle Dispersion for Carbon/Carbon Composites , WILEY-V C H VERLAG GMBH,2008,10(10),986-989 ,DOI:10.1002/adem.200800016, ISSN:1438-1656
807. Microstructure and oxidation protective ability of MoSi2-SiC-Si coating toughened with SiC whiskers for carbon/carbon composites , MANEY PUBLISHING,2008,24(5),383-387 ,DOI:10.1179/174329408X326425, ISSN:0267-0844
808. Isotropic pyrocarbon deposited at 1250 degrees C by means of thermal gradient chemical vapor deposition , ELSEVIER SCIENCE BV,2009,384(3),327-329 ,DOI:10.1016/j.jnucmat.2008.11.004, ISSN:0022-3115
809. A Si-Mo-W Coating to Protect SiC-Coated Carbon/Carbon Composites Against Oxidation , WILEY-BLACKWELL,2009,92(9),2132-2135 ,DOI:10.1111/j.1551-2916.2009.03144.x, ISSN:0002-7820
810. B2O3 modified SiC-MoSi2 oxidation resistant coating for carbon/carbon composites by a two-step pack cementation , PERGAMON-ELSEVIER SCIENCE LTD,2009,51(10),2450-2454 ,DOI:10.1016/j.corsci.2009.06.033, ISSN:0010-938X
811. A MoSi2-SiC-Si/MoSi2 COATING TO PROTECT CARBON/CARBON COMPOSITES AGAINST OXIDATION AT 1700 degrees C , WORLD SCIENTIFIC PUBL CO PTE LTD,2009,16(3),437-440 ,DOI:10.1142/S0218625X09012822, ISSN:0218-625X
812. Bamboo-shaped carbon nanofibers obtained in pyrolytic carbon by thermal gradient chemical vapor deposition , PERGAMON-ELSEVIER SCIENCE LTD,2009,47(10),2540-2542 ,DOI:10.1016/j.carbon.2009.05.010, ISSN:0008-6223
813. OXIDATION RESISTANT (Mo,W)Si-2 COATING FOR SiC-COATED CARBON/CARBON COMPOSITES BY IN SITU FORMATION METHOD , WORLD SCIENTIFIC PUBL CO PTE LTD,2009,16(2),309-313 ,DOI:10.1142/S0218625X09012640, ISSN:0218-625X
814. Mo-Si-B ALLOYS OXIDATION PROTECTIVE COATING FOR SiC-COATED CARBON/CARBON COMPOSITES , WORLD SCIENTIFIC PUBL CO PTE LTD,2009,16(2),223-229 ,DOI:10.1142/S0218625X09012524, ISSN:0218-625X
815. Fabrication of Isotropic Pyrocarbon at 1400 degrees C by Thermal Gradient Chemical Vapor Deposition Apparatus , JOURNAL WUHAN UNIV TECHNOLOGY,2009,24(5),728-731 ,DOI:10.1007/s11595-009-5728-7, ISSN:1000-2413
816. 密度和纤维取向对炭/炭复合材料烧蚀性能的影响 , SCIENCE CHINA PRESS,2010,25(3),161-167 ,DOI:10.1016/S1872-5805(09)60023-8, ISSN:1007-8827
817. Multilayer oxidation protective coating for C/C composites from room temperature to 1500 degrees C , ELSEVIER SCIENCE SA,2010,204(11),1831-1835 ,DOI:10.1016/j.surfcoat.2009.11.026, ISSN:0257-8972
818. C/C复合材料高温抗氧化涂层的研究现状与展望 , SCIENCE CHINA PRESS,2010,25(04),337-343 ,DOI:10.3724/SP.J.1077.2010.00337, ISSN:1000-324X
819. 2D C/C复合材料微观结构与力学性能的研究 , SCIENCE PRESS,2010,25(2),173-176 ,DOI:10.3724/SP.J.1077.2010.00173, ISSN:1000-324X
820. Effect of interface structures on the fracture behavior of two-dimensional carbon/carbon composites by isothermal chemical vapor infiltration , SPRINGER,2010,45(6),1432-1437 ,DOI:10.1007/s10853-009-4089-0, ISSN:0022-2461
821. Multi-physical field coupling simulation of TCVI process for preparing carbon/carbon composites , SCIENCE PRESS,2009,52(11),3173-3179 ,DOI:10.1007/s11431-009-0126-0, ISSN:1006-9321
822. Microstructure and oxidation resistant property of C/C composites modified by SiC-MoSi2-CrSi2 coating , MANEY PUBLISHING,2011,27(5),355-361 ,DOI:10.1179/026708410X12687356948670, ISSN:0267-0844
823. SiC nanowires reinforced MAS joint of SiC coated carbon/carbon composites to LAS glass ceramics , ELSEVIER SCIENCE SA,2012,532,255-259 ,DOI:10.1016/j.msea.2011.10.088, ISSN:0921-5093
824. Oxidation resistant Si-Mo-Al coating for C/SiC coated carbon/carbon composites at high temperature , MANEY PUBLISHING,2012,28(4),257-260 ,DOI:10.1179/1743294411Y.0000000041, ISSN:0267-0844
825. Mechanical properties enhancement of carbon/carbon composites by in situ grown carbon nanofibers , ELSEVIER SCIENCE SA,2012,547,138-141 ,DOI:10.1016/j.msea.2012.03.083, ISSN:0921-5093
826. The preparation and mechanical properties of carbon-carbon/lithium-aluminum-silicate composite joints , Elsevier Ltd,2013,44,346-353 ,DOI:10.1016/j.matdes.2012.07.063, ISSN:02641275
827. A Si-SiC Oxidation-resistant Coating for Carbon/Carbon Composites by Hot-pressing Reaction Technique , WILEY-BLACKWELL,2014,11(2),342-349 ,DOI:10.1111/ijac.12014, ISSN:1546-542X
828. PREPARATION AND ELECTROCHEMICAL CAPACITIVE BEHAVIOR OF GRAPHENE BY MICROWAVE ASSISTED THERMAL REDUCTION OF GRAPHITE OXIDE IN HYDRAZINE HYDRATE , WORLD SCIENTIFIC PUBL CO PTE LTD,2014,9(6) ,DOI:10.1142/S1793292014500660, ISSN:1793-2920
829. 蒙脱土改性炭泡沫复合材料 , ELSEVIER SCIENCE BV,2014,29(2),143-148 ,DOI:10.3969/j.issn.1007-8827.2014.02.013, ISSN:1007-8827
830. 浸渍用有机聚锆前驱体的制备与表征 , SCIENCE PRESS,2014,(1),56-62 ,DOI:10.3724/SP.J.1105.2014.13155, ISSN:1000-3304
831. 溶胶-凝胶法制备HfB2粉体及其氧化行为 , NORTHWEST INST NONFERROUS METAL RESEARCH,2013,42(12),2594-2597 ,DOI:, ISSN:1002-185X
832. 弯曲疲劳后4D-C/C复合材料的抗弯强度及热膨胀性能(英文) , ELSEVIER SCIENCE BV,2014,29(03),169-175 ,DOI:10.1016/S1872-5805(14)60132-3, ISSN:1007-8827
833. Influence of Chromium Content on the Oxidation Resistance of Al-Si Alloy Coating for SiC Coated Carbon-Carbon Composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2010,39,544-547 ,DOI:, ISSN:1002-185X
834. SiC nanowire-toughened SiC-MoSi2-CrSi2 oxidation protective coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2010,205(2),413-418 ,DOI:10.1016/j.surfcoat.2010.07.001, ISSN:0257-8972
835. 热解炭过渡层-中间相沥青基炭/炭复合材料的微观结构 , SCIENCE CHINA PRESS,2010,25(4),297-302 ,DOI:, ISSN:1007-8827
836. Study on the thermal expansion properties of C/C composites , SPRINGER,2007,42(10),3435-3439 ,DOI:10.1007/s10853-006-1123-3, ISSN:0022-2461
837. Si-Mo-Cr coating for C/SiC coated carbon/carbon composites against oxidation , MANEY PUBLISHING,2012,28(7),544-547 ,DOI:10.1179/1743294412Y.0000000005, ISSN:0267-0844
838. C/C复合材料与镍基高温合金连接接头的力学性能和微观结构 , NORTHWEST INST NONFERROUS METAL RESEARCH,2011,40(1),111-114 ,DOI:, ISSN:1002-185X
839. 等离子喷涂法制备炭/炭复合材料硅酸钇涂层研究 , SCIENCE CHINA PRESS,2010,25(3),187-191 ,DOI:, ISSN:1007-8827
840. 3D C/C复合材料的热膨胀性能 , SCIENCE PRESS,2010,25(1),60-64 ,DOI:, ISSN:1007-8827
841. Effect of Thermal Shock and Oxidation on Mechanical Property of Carbon/Carbon Composites with a Silicide Coating , NORTHWEST INST NONFERROUS METAL RESEARCH,2009,38,37-40 ,DOI:, ISSN:1002-185X
842. 原位聚合法制备酚醛树脂空心微球的工艺研究及性能表征 , SCIENCE PRESS,2009,(7),695-699 ,DOI:, ISSN:1000-3304
843. A Si-SiC oxidation protective coating for carbon/carbon composites prepared by a two-step pack cementation , ELSEVIER SCI LTD,2009,35(6),2525-2529 ,DOI:10.1016/j.ceramint.2009.01.005, ISSN:0272-8842
844. Si-Al-Ir Oxidation Resistant Coating for Carbon/Carbon Composites by Slurry Dipping , JOURNAL MATER SCI TECHNOL,2009,25(3),344-346 ,DOI:, ISSN:1005-0302
845. Preparation of phenolic hollow microspheres via in situ polymerization , JOHN WILEY & SONS LTD,2009,58(5),465-468 ,DOI:10.1002/pi.2567, ISSN:0959-8103
846. C/C复合材料防氧化涂层SiC/SiC-MoSi2的制备与抗氧化性能 , SCIENCE PRESS,2009,45(4),503-506 ,DOI:10.3321/j.issn:0412-1961.2009.04.021, ISSN:0412-1961
847. Influence of Thermal Shock on the Mechanical Behavior of Si-SiC Coated Carbon/Carbon Composites , JOURNAL MATER SCI TECHNOL,2009,25(2),251-253 ,DOI:, ISSN:1005-0302
848. 短切炭纤维的表面处理对沥青基C/C复合材科性能的影响 , SCIENCE PRESS,2009,24(1),89-92 ,DOI:, ISSN:1007-8827
849. 不同氧化物对C/C复合材料SiC涂层性能的影响 , SCIENCE PRESS,2009,24(1),45-49 ,DOI:, ISSN:1007-8827
850. Study of fluorhydroxyapatite coatings on carbon/carbon composites , ELSEVIER SCIENCE SA,2009,203(13),1771-1775 ,DOI:10.1016/j.surfcoat.2008.12.009, ISSN:0257-8972
851. The Infiltration Process and Texture Transition of 2D C/C Composites , JOURNAL MATER SCI TECHNOL,2009,25(1),109-114 ,DOI:, ISSN:1005-0302
852. 炭/炭复合材料表面预炭层的制备及其性能研究 , SCIENCE PRESS,2009,24(1),125-128 ,DOI:10.3724/SP.J.1077.2009.00125, ISSN:1000-324X
853. Effect of chemical vapor infiltration treatment on the wave-absorbing performance of carbon fiber/cement composites , INT JOURNAL MINERALS METALLURGY & MATERIALS, EDITORIAL DEPT,2008,15(6),808-815 ,DOI:, ISSN:1005-8850
854. 碳泡沫导热性能及力学性能研究 , SCIENCE CHINA PRESS,2008,23(6),1171-1174 ,DOI:10.3321/j.issn:1000-324X.2008.06.017, ISSN:1000-324X
855. C/SiC/Si-Mo-Cr复合涂层碳/碳复合材料力学性能研究 , SCIENCE CHINA PRESS,2008,23(4),725-728 ,DOI:10.3321/j.issn:1000-324X.2008.04.018, ISSN:1000-324X
856. 溴插层热解炭的制备 , SCIENCE CHINA PRESS,2008,23(2),185-188 ,DOI:, ISSN:1007-8827
857. Carbon composites reinforced by graphite grains , ELSEVIER SCIENCE BV,2008,375(2),280-282 ,DOI:10.1016/j.jnucmat.2007.12.004, ISSN:0022-3115
858. 粒状增强体种类对沥青基炭复合材料性能的影响 , SCIENCE CHINA PRESS,2008,23(1),51-57 ,DOI:10.1016/S1872-5805(08)60012-8, ISSN:1007-8827
859. 炭纤维针刺预制体增强C/SiC复合材料的制备与性能研究 , SCIENCE CHINA PRESS,2008,23(2),223-228 ,DOI:10.3321/j.issn:1000-324X.2008.02.004, ISSN:1000-324X
860. Structure and oxidation Behavior of a plasma sprayed yttrium silicates coated SiC-C/C with a glass outer sealant from 1573K to 1873K , JOURNAL WUHAN UNIV TECHNOLOGY,2008,23(1),33-37 ,DOI:10.1007/s11595-006-1033-x, ISSN:1000-2413
861. Effects of tensile fatigue loads on flexural behavior of 3D braided C/C composites , ELSEVIER SCI LTD,2008,68(2),333-336 ,DOI:10.1016/j.compscitech.2007.10.040, ISSN:0266-3538
862. The mechanism of effect of ultrasonic on the apatite bioactive coating for C/C composites by sonoelectrodeposition , NORTHWEST INST NONFERROUS METAL RESEARCH,2007,36,594-598 ,DOI:, ISSN:1002-185X
863. Effects of catalyst content on matrices of C/C composites by chemical liquid-vapor in-filtration , NORTHWEST INST NONFERROUS METAL RESEARCH,2007,36,530-534 ,DOI:, ISSN:1002-185X
864. Microstructure and mechanical properties of mesophase pitch-based C/C composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2007,36,331-334 ,DOI:, ISSN:1002-185X
865. Effect of the pore-forming agent and silicon powders size on the properties of RBSN , NORTHWEST INST NONFERROUS METAL RESEARCH,2007,36,269-272 ,DOI:, ISSN:1002-185X
866. Oxidation behavior of SiC nanoparticle-SiC oxidation protective coating for carbon/carbon composites at 1773 K , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(13),2704-2707 ,DOI:10.1016/j.carbon.2007.08.013, ISSN:0008-6223
867. 碳纤维增强水泥基复合材料电磁性能的研究 , NORTHWEST INST NONFERROUS METAL RESEARCH,2007,36(10),1702-1708 ,DOI:10.3321/j.issn:1002-185x.2007.10.003, ISSN:1002-185X
868. Influence of NaF concentration on fluorine-containing hydroxyapatite coating on carbon/carbon composites , ELSEVIER SCIENCE SA,2007,106(1),22-26 ,DOI:10.1016/j.matchemphys.2007.05.013, ISSN:0254-0584
869. 包埋浸渗/气相沉积二步法在C/C复合材料表面制备SiC涂层 , SCIENCE CHINA PRESS,2007,22(4),737-741 ,DOI:10.3321/j.issn:1000-324x.2007.04.034, ISSN:1000-324X
870. W-Mo-Si/SiC oxidation protective coating for carbon/carbon composites , JOURNAL MATER SCI TECHNOL,2007,23(4),559-562 ,DOI:, ISSN:1005-0302
871. Preparation of well-aligned carbon nanotubes by pyrolysis of phenolic resin in anodic alumina pores , ELSEVIER SCIENCE BV,2007,253(18),7365-7368 ,DOI:10.1016/j.apsusc.2007.03.028, ISSN:0169-4332
872. Oxidation resistant yttrium silicates coating for carbon/carbon composites prepared by a novel in-situ formation method , ELSEVIER SCI LTD,2007,33(5),887-890 ,DOI:10.1016/j.ceramint.2006.01.007, ISSN:0272-8842
873. A Si-Mo oxidation protective coating for C/SiC coated carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(5),1130-1133 ,DOI:10.1016/j.carbon.2006.12.028, ISSN:0008-6223
874. A Cr-Al-Si oxidation resistant coating for carbon/carbon composites by slurry dipping , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(5),1124-1126 ,DOI:10.1016/j.carbon.2007.01.010, ISSN:0008-6223
875. High performance Si-SiC composite coating for C/C composites prepared by a two-step pack cementation process , WILEY-V C H VERLAG GMBH,2007,9(4),322-324 ,DOI:10.1002/adem.200600235, ISSN:1438-1656
876. 一种新型C/C复合材--石墨粉增强热解炭 , SCIENCE CHINA PRESS,2007,22(1),12-16 ,DOI:10.3321/j.issn:1007-8827.2007.01.003, ISSN:1007-8827
877. A SiC/glass oxidation protective coating for carbon/carbon composites for application at 1173 K , PERGAMON-ELSEVIER SCIENCE LTD,2007,45(4),892-894 ,DOI:10.1016/j.carbon.2006.12.014, ISSN:0008-6223
878. The effect of applied stress on damage mode of 3D C/C composites under bend-bend fatigue loading , SCIENCE CHINA PRESS,2007,50(1),97-102 ,DOI:10.1007/s11431-007-2025-6, ISSN:1006-9321
879. A C/SiC gradient oxidation protective coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2006,201(6),3491-3495 ,DOI:10.1016/j.surfcoat.2006.07.239, ISSN:0257-8972
880. Silicide coating for protection of C/C composites at 1873 K , ELSEVIER SCIENCE SA,2006,201(6),3082-3086 ,DOI:10.1016/j.surfcoat.2006.06.022, ISSN:0257-8972
881. A SiC whisker-toughened SiC-CrSi2 oxidation protective coating for carbon/carbon composites , ELSEVIER SCIENCE BV,2007,253(8),3757-3760 ,DOI:10.1016/j.apsusc.2006.07.092, ISSN:0169-4332
882. Effect of SiC whiskers on the microstructure and oxidation protective ability of SiC-CrSi2 coating for carbon/carbon composites , ELSEVIER SCIENCE SA,2007,445,386-391 ,DOI:10.1016/j.msea.2006.09.067, ISSN:0921-5093
883. 高温退火一步非破坏性纯化碳纳米管 , SCIENCE CHINA PRESS,2006,64(23),2365-2368 ,DOI:10.3321/j.issn:0567-7351.2006.23.012, ISSN:0567-7351
884. AMOSi(2)-SiC-Si/glass oxidation protective coating for carbon/carbon composites , PERGAMON-ELSEVIER SCIENCE LTD,2006,44(15),3361-3364 ,DOI:10.1016/j.carbon.2006.08.024, ISSN:0008-6223
885. Study on the thermal fatigue behavior of SiC coated carbon/carbon composites , ELSEVIER SCIENCE SA,2006,434(1-2),335-338 ,DOI:10.1016/j.msea.2006.07.031, ISSN:0921-5093
886. Ablation behavior of HfC modified carbon/carbon composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2006,35,365-368 ,DOI:, ISSN:1002-185X
887. Fracture characteristics of carbon/carbon composites prepared by mix technics , NORTHWEST INST NONFERROUS METAL RESEARCH,2006,35,245-248 ,DOI:, ISSN:1002-185X
888. 碳化硅-碳/碳复合材料表面掺铬碳膜的研究 , NORTHWEST INST NONFERROUS METAL RESEARCH,2006,35(8),1204-1207 ,DOI:10.3321/j.issn:1002-185X.2006.08.007, ISSN:1002-185X
889. 炭/炭复合材料声电沉积钙磷生物活性涂层的生长机理 , NORTHWEST INST NONFERROUS METAL RESEARCH,2006,35(7),1096-1100 ,DOI:10.3321/j.issn:1002-185X.2006.07.020, ISSN:1002-185X
890. 脉冲FCVI制备炭/炭复合材料的微观结构及力学性能 , SCIENCE CHINA PRESS,2006,21(2),132-138 ,DOI:10.3321/j.issn:1007-8827.2006.02.007, ISSN:1007-8827
891. SiC whisker-toughened MoSi2-SiC-Si coating to protect carbon/carbon composites against oxidation , PERGAMON-ELSEVIER SCIENCE LTD,2006,44(9),1866-1869 ,DOI:10.1016/j.carbon.2006.03.002, ISSN:0008-6223
892. Influence of preparation technology on the microstructure and anti-oxidation property of SiC-Al2O3-mullite multi-coatings for carbon/carbon composites , ELSEVIER SCIENCE BV,2006,252(12),4244-4249 ,DOI:10.1016/j.apsusc.2005.07.004, ISSN:0169-4332
893. Yttrium silicate oxidation protective coating for SiC coated carbon/carbon composites , ELSEVIER SCI LTD,2006,32(4),417-421 ,DOI:10.1016/j.ceramint.2005.03.018, ISSN:0272-8842
894. Preparation and oxidation kinetics mechanism of three-layer multi-layer-coatings-coated carbon/carbon composites , ELSEVIER SCIENCE SA,2006,200(18-19),5379-5385 ,DOI:10.1016/j.surfcoat.205.06.011, ISSN:0257-8972
895. 短切炭纤维增强沥青基C/C复合材料的力学性能 , SCIENCE PRESS,2006,21(01),36-42 ,DOI:10.3321/j.issn:1007-8827.2006.01.007, ISSN:1007-8827
896. Microstructure and anti-oxidation property of CrSi2-SiC coating for carbon/carbon composites , ELSEVIER SCIENCE BV,2006,252(10),3475-3480 ,DOI:10.1016/j.apsusc.2005.05.018, ISSN:0169-4332
897. Effect of SiC whiskers on the oxidation protective properties of SiC coatings for carbon/carbon composites , NONFERROUS METALS SOCIETY CHINA,2006,25(1),58-62 ,DOI:10.1016/S1001-0521(06)60015-6, ISSN:1001-0521
898. New application of intercalation on improving toughness of carbon/carbon composites , ELSEVIER SCIENCE SA,2006,96(2-3),376-380 ,DOI:10.1016/j.matchemphys.2005.07.027, ISSN:0254-0584
899. 炭/炭复合材料高温抗氧化涂层的研究进展 , SCIENCE PRESS,2005,20(4),373-379 ,DOI:10.3321/j.issn:1007-8827.2005.04.016, ISSN:1007-8827
900. Si-SiC oxidation protective coating for carbon/carbon composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2005,34,261-264 ,DOI:, ISSN:1002-185X
901. Silicon carbide coating to protect carbon/carbon composites against oxidation , PERGAMON-ELSEVIER SCIENCE LTD,2005,52(9),923-927 ,DOI:10.1016/j.scriptamat.2005.12.029, ISSN:1359-6462
902. Preparation and oxidation kinetics of SiC/ZrO2-SiO2 oxidation protective coating for carbon-carbon composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2005,34,324-328 ,DOI:, ISSN:1002-185X
903. Oxidation behavior of SiC-Al2O3-mullite multi-coating coated carbon/carbon composites at high temperature , PERGAMON-ELSEVIER SCIENCE LTD,2005,43(7),1580-1583 ,DOI:10.1016/j.carbon.2005.01.033, ISSN:0008-6223
904. Numerical simulation of chemical vapor infiltration of propylene into C/C composites with reduced multi-step kinetic models , PERGAMON-ELSEVIER SCIENCE LTD,2005,43(14),2937-2950 ,DOI:10.1016/j.carbon.2005.05.046, ISSN:0008-6223
905. 压力梯度CVI工艺制备2D炭/炭复合材料的弯曲断裂行为 , SCIENCE CHINA PRESS,2004,19(4),289-292 ,DOI:10.3321/j.issn:1007-8827.2004.04.008, ISSN:1007-8827
906. 焦炭颗粒的平均细度对沥青基炭复合材料性能的影响 , SCIENCE PRESS,2005,20(3),235-239 ,DOI:10.3321/j.issn:1007-8827.2005.03.008, ISSN:1007-8827
907. Effect of molybdenum and tungsten on reactive joint of carbon-carbon composites , NORTHWEST INST NONFERROUS METAL RESEARCH,2005,34,365-367 ,DOI:, ISSN:1002-185X
908. 碳/碳复合材料表面声电沉积/碱热处理复合工艺制备羟基磷灰石生物活性涂层研究 , NORTHWEST INST NONFERROUS METAL RESEARCH,2005,34(9),1489-1492 ,DOI:10.3321/j.issn:1002-185X.2005.09.036, ISSN:1002-185X
909. 人工神经网络建模在抗烧蚀炭/炭复合材料基体改性研究中的应用 , SCIENCE CHINA PRESS,2004,19(4),275-280 ,DOI:10.3321/j.issn:1007-8827.2004.04.006, ISSN:1007-8827
910. 沥青过渡层对C/C复合材料力学性能的影响 , Chinese Journal of Materials Research,2006,20(4),381-385 ,DOI:10.3321/j.issn:1005-3093.2006.04.008, ISSN:1005-3093
911. 中间相沥青基碳/碳复合材料的组织与性能 , Beijing Institute of Aeronautical Materials (BIAM), Beijing, China,2006,(5),21-24 ,DOI:10.3969/j.issn.1001-4381.2006.05.005, ISSN:1001-4381
912. C/C复合材料与LAS陶瓷连接的显微结构与性能 , 2008,23(4),13-16 ,DOI:10.3969/j.issn.1003-1545.2008.04.004, ISSN:1003-1545
913. 炭化压力对中间相沥青焦微观结构的影响 , 2010,31(5),4-7 ,DOI:10.3969/j.issn.1672-6871.2010.05.002, ISSN:1672-6871
914. Effects of microstructures on the ablation behaviors of ZrC deposited by CVD , Elsevier, P.O. Box 211, Amsterdam, 1000 AE, Netherlands,2014,240,450-455 ,DOI:10.1016/j.surfcoat.2013.12.074, ISSN:02578972
915. Synthesis and characterization of nanobelt-shaped Na, F and carbonate multi-substituted hydroxyapatite , Elsevier,2014,138,48-51 ,DOI:10.1016/j.matlet.2014.09.099, ISSN:0167577X
916. Effect of SiC Location on the Ablation of C/C-SiC Composites in Two Heat Fluxes , JOURNAL MATER SCI TECHNOL,2015,31(4),345-354 ,DOI:10.1016/j.jmst.2014.11.021, ISSN:1005-0302
917. Flexural fatigue behavior of 2D cross-ply carbon/carbon composites at room temperature , ELSEVIER SCIENCE SA,2015,634,209-214 ,DOI:10.1016/j.msea.2015.03.029, ISSN:0921-5093
918. Ablation behavior and mechanism of C/C-HfC-SiC composites , PERGAMON-ELSEVIER SCIENCE LTD,2015,116,124-129 ,DOI:10.1016/j.vacuum.2015.03.024, ISSN:0042-207X
919. 国内外C/C复合材料疲劳性能的研究进展 , 2010,(中国浙江宁波),5 ,DOI:, ISSN:
920. 热梯度CVI工艺制备炭/炭复合材料管型件(英文) , 2006,(S1),345-348 ,DOI:, ISSN:1001-4381
921. 炭/炭复合材料热梯度化学气相沉积工艺 , 2004,(中国北京),1 ,DOI:, ISSN:
922. 热梯度化学气相沉积制备炭/炭复合材料制件 , 2004,(中国海口),120-123 ,DOI:, ISSN:
923. 碳纤维增强纸基摩擦材料磨损机理研究 , 2011,(中国北京),400-405 ,DOI:, ISSN:

社会兼职 Social Appointments